MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Glyptal G1228 High-Gloss Enamel
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: GLYPTAL 1228 is a high-gloss enamel for general finishing of machinery and electrical apparatus. It has excellent outdoor durability and high resistance to transformer oils. It may be used on primed metal or wood surfaces. Also available in aerosol (G1228A).

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³
Solids Content 40 %40 %Volume
 56 %56 %Weight
Fineness >= 7.0>= 7.0Hegman
 
Mechanical PropertiesMetricEnglishComments
Impact Test 4.07 J3.00 ft-lbDirect Impact Resistance
 4.07 J3.00 ft-lbIndirect Impact Resistance
 
Thermal PropertiesMetricEnglishComments
Flash Point 28.9 °C84.0 °FOpen Cup
 
Optical PropertiesMetricEnglishComments
Gloss >= 85 %>= 85 %60°
 
Processing PropertiesMetricEnglishComments
Dry Time 12.0 hour12.0 hourHandle
 16.0 hour16.0 hourRecoat
Tack-Free Time 360 min6.00 hour
 
Descriptive Properties
AdhesionExcellentCross Hatch
Color#49 ASA Gray
Coverage600-700 ft²/gal1 mil dry film thickness
FlexibilityPass 180°1/8" Mandrel
MethodSpray, brush, or roller
Pencil Hardness2B
ReducerMineral Spirits (G2085)For brush or roller
 Xylol (G3190)For spray
Solvent SystemAliphatic/Aromatic
SubstrateFerrous metal primed with G7635
Viscosity67-77 KU

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay GEROPON® SDS Surfactant
Shandong Rike Chemical ACM-2 PVC Impact Modifier ACM Resin
Saint-Gobain Rulon® ACM Bearing/Seal PTFE
Plastcom SLOVASTER® B/A GF 20 PBT, 20% glass fibre
Lanxess Rhenogran® KST-50/ACM (GE 1857) Rubber Processing Aid

PGLYPT929 / 209768

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.