MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecapeek® PVX Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: TECAPEEK® PVX is an ultra high performance bearing material made from Victrex® PEEK polymer. TECAPEEK® PVX incorporates the properties of a premium polymetric matrix material with optimum levels of specific wear enhancing additives. This formulation raises the continuous use temperature by approximately 40°F and increases the limiting PV while maintaining excellent chemical resistance. When used as a non-metallic bearing, TECAPEEK® PVX offers a good range of tribological performance. It is designed to run at high loads and speeds, in hostile environments, either dry or lubricated.
  • Continuous use temperature over 450°F
  • Flammability is UL94 V-O with a low limiting O2 index (-40%) and very low smoke generation
  • Can be used dry against hard or soft mating surfaces
  • Excellent weather resistance
  • Resistant to gamma radiation
  • Complies with specific provisions of ASTM D6262-98
  • Available in a wide range of sizes, extruded in rod and plate for subsequent machined parts

TECAPEEK® PVX great properties make it an ideal material for bearing surfaces in the most demanding applications and in the harshest conditions. Industrial, automotive, marine, nuclear, petroleum and aerospace industry applications realize great benefits from its use.

Information Provided by Ensinger Inc.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.48 g/cc1.48 g/ccASTM D792
Density 1.48 g/cc0.0535 lb/in³ASTM D792
Water Absorption <= 0.10 %
@Temperature 22.8 °C,
Time 86400 sec
<= 0.10 %
@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570
Water Absorption at Saturation 0.10 %0.10 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585
Tensile Strength, Yield 119 MPa17300 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Tensile Modulus 8.96 GPa1300 ksiASTM D638
Flexural Strength 207 MPa30000 psiASTM D790
Flexural Modulus 8.27 GPa1200 ksiASTM D790
 9.65 GPa
@Temperature 22.8 °C
1400 ksi
@Temperature 73.0 °F
Tangent; ASTM D790
Compressive Strength 152 MPa22000 psiASTM D695
Izod Impact, Notched 0.854 J/cm1.60 ft-lb/inASTM D256
 1.74 J/cm
@Temperature 22.8 °C
3.25 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Coefficient of Friction, Dynamic 0.19
@Pressure 0.276 MPa
0.19
@Pressure 40.0 psi
50 fpm
Coefficient of Friction, Static 0.23
@Pressure 0.276 MPa
0.23
@Pressure 40.0 psi
K Factor (Wear Factor) 1.25 - 1.51.25 - 1.5in/min x 10-3
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1e+05 - 1.00e+8 ohm1e+05 - 1.00e+8 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.0 µm/m-°C15.0 µin/in-°F
Melting Point 334 °C633 °F
Maximum Service Temperature, Air 260 °C500 °Fcontinuous
Deflection Temperature at 1.8 MPa (264 psi) 277 °C530 °FASTM D648
Flammability, UL94 V-0V-0
 
Descriptive Properties
Base MaterialPEEK
Maximum PV25000-30000

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Overview of materials for Polyetheretherketone, Unreinforced
Ensinger Tecapeek® CF30 Polyetheretherketone, 30% Carbon Reinforced (PEEK)
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone

PENSIN005 / 92822

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.