MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BCC Products Kwik Kast BC 8645 Urethane Casting
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: BCC Kwik Kast/Gray is a two component, fast setting polyurethane reproduction plastic. BC8645 has been reformulated to enhance filler suspension and avoid hard packing @ 77ºF. Uses include; tracing models, core boxes, duplicating aids, patterns, prototypes, low temperature vacuum form tools, etc.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 - 1.90 g/ccASTM D792-66
Brookfield Viscosity 2075 cP#3 spindle @ 20 rpm; ASTM D2393
Linear Mold Shrinkage 0.00080 cm/cmASTM D2566-69
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
@Temperature 23.9 °C
ASTM D2240
Tensile Strength, Ultimate 4875 psiASTM D638
Flexural Strength 6250 psi
Compressive Strength 9600 psiASTM D695
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 174 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 - 120 min
@Temperature 25.0 °C
demold time
Pot Life 5.0 - 6.0 min
@Temperature 25.0 °C
1 lb. mass
 
Descriptive Properties
Mix Ratio1:1 by weight or volume
Wear Resistance (Tabor Method)Very Good

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BCC Products Kwik Kast BC 8650 Urethane Casting
BCC Products METAL-KAST BC 8010 Urethane Casting
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting
BCC Products SLO-KAST BC 8009 Urethane Casting
BCC Products BC 8870 Polyurethane Elastomer

PBCC048 / 107275

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.