MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Corning Vycor® 7904 Blue Glass  (discontinued **)
Categories: Ceramic; Glass; Optical; Oxide; Silicon Oxide

Material Notes: Absorbs yellow wavelengths and causes light transmitted through the glass to have a higher color temperature. Cobalt is introduced into the glass structure; therefore a lamp can be produced without the issues of burn-off and light scatter that coated lamps have. Blue VYCOR can be run in high temperature lamp manufacturing processes without additional cost or process steps.

Special Features:

  • Superior optical quality
  • Tight dimensional control
  • Thermal and chemical properties ideally suited to high temperatures.
  • Excellent thermal shock resistance

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
CTE, linear 0.850 µm/m-°C
@Temperature 20.0 °C
0.472 µin/in-°F
@Temperature 68.0 °F
Softening Point 1005 °C1841 °F
Annealing Point 900 °C1650 °F
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  53 - 61 %
@Thickness 1.00 mm,
Wavelength 590 nm
53 - 61 %
@Thickness 0.0394 in,
Wavelength 590 nm
tubing
 62 - 70 %
@Thickness 1.00 mm,
Wavelength 500 nm
62 - 70 %
@Thickness 0.0394 in,
Wavelength 500 nm
tubing
 82 - 90 %
@Thickness 1.00 mm,
Wavelength 400 nm
82 - 90 %
@Thickness 0.0394 in,
Wavelength 400 nm
tubing
IR Transmittance 92 %
@Thickness 1.00 mm,
Wavelength 800 nm
92 %
@Thickness 0.0394 in,
Wavelength 800 nm
tubing
UV Transmittance  <= 1.0 %
@Thickness 1.00 mm,
Wavelength 200 nm
<= 1.0 %
@Thickness 0.0394 in,
Wavelength 200 nm
tubing
 73 %
@Thickness 1.00 mm,
Wavelength 300 nm
73 %
@Thickness 0.0394 in,
Wavelength 300 nm
tubing
 
Component Elements PropertiesMetricEnglishComments
SiO2 96 %96 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borosilicate Glass
Overview of materials for Polyphenylene Sulfide (PPS); Molded
96% Silica Consolidated Reconstructed Glass
A. Schulman POLYBATCH™ Blue 4012 Concentrate Based in Polyethylene
Corning Gorilla® Glass 2

CCORNV00 / 746

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.