MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Acetic Acid (CH3CO2H; Ethanoic Acid)
Categories: Fluid; Solvent

Key Words: CH3CO2H
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.0492 g/cc
@Temperature 20.0 °C
Viscosity 1.056 cP
@Temperature 25.0 °C
Molecular Weight 60.05 g/mol
Vapor Pressure 0.09869 atm
@Temperature 55.9 °C
 11.325 torr
@Temperature 20.0 °C
Surface Tension 27.1 dynes/cmat 25°C; Gamma
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 57.103 atm
Critical Temperature 319.55 °C
Critical Density 0.351 g/cc
Critical Molar Volume 171 cm³/mol
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 6.17
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 195.3 J/gEnthalpy of fusion at normal melting point
Heat of Vaporization 394.3 J/g
 394.7 J/gEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 2.05 J/g-°C
 1.108 J/g-°C
@Temperature 25.0 °C
Vapor
Thermal Conductivity 0.158 W/m-K
@Temperature 25.0 °C
Melting Point 16.64 °CAt atmospheric pressure (760 torr)
 16.65 °C
Boiling Point 17.0 °Cat 10 torr
 117.9 °C
@Pressure 0.101 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.3716
@Temperature 20.0 °C,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.808
Antoine's Vapor Pressure B Parameter3405.57
Antoine's Vapor Pressure C Parameter-56.34
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)64-19-7
Chemical FormulaCH3COOH
Critical Compressibility (Zc)0.2
Dipole moment (p/C.m)4.336E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A600.94
Dynamic Viscosity Parameter B306.21
Henry's Law Constant (atm m3/mol)4.42E-05
Molar Heat Capacity (298K)66.508 J/mol-K
Molar Heat Capacity of Vapor a Parameter4.8367
Molar Heat Capacity of Vapor b Parameter0.2547
Molar Heat Capacity of Vapor c Parameter-0.0001752
Molar Heat Capacity of Vapor d Parameter4.945E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UV cut-off (nm)260

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese 50000990 FOOD GRADE 80% Acetic Acid
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
1-Pentanol, C5H12O

VORG000 / 74511

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.