MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Pyrotek Hirolex HG Electrical Insulating Material
Categories: Ceramic

Material Notes: Hirolex HG has superior mechanical properties. It is highly resistant to thermal shock, non-flammable and offers good arc resistance.

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.95 g/cc1.95 g/cc
Water Absorption 0.50 %0.50 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 303 MPa43900 psi
Compressive Strength 379 MPa55000 psi
Izod Impact, Notched 16.0 J/cm30.0 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 10.0 kV/mm254 kV/in
Arc Resistance 260 sec260 sec
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.360 W/m-K2.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 250 °C482 °FContinuous use
 510 °C950 °F
Flammability, UL94 V-0V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crystex Composites Mykroy/Mycalex 555 Molding Grade Glass-bonded Mica Composite
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Pyrotek MCX-40 Insulating Board
Overview of materials for Nylon 66, 60% Glass Fiber Filled
Overview of materials for Nylon 610

CPYRO147 / 1868

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.