MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek MCX-40 Insulating Board
Categories: Ceramic

Material Notes: MCX-40 is a bonded-mica composite for use in glass contact applications. Its high operating temperature, low porosity, and low thermal conductivity make it ideal for all areas of hot glass transfer, including takeout jaws/inserts, sweep out pads, lehr loader bar pads/inserts, and high temperature flat glass quench rollers.

Applications

  • Glass contact insulating material

Advantages

  • Abrasion resistant
  • Non-marking to glass
  • Low porosity
  • Resists oxidizing atmospheres better than carbon or graphite
  • Machinable with standard equipment
  • High-impact strength
  • Can be molded to net shape based on consumer specifications

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.491 g/cc0.08999 lb/in³
Water Absorption 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 90.0 MPa13100 psi
Compressive Strength 310 MPa45000 psi
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.420 W/m-K2.91 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 510 °C950 °FContinuous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek B-3A REFRACTORY BOARD
Pyrotek ISOMAG® 45 Thermal Insulation Board
Pyrotek EZ-400 Refractory Coating
Pyrotek Bonded Particle Filtration Media
Pyrotek ISOCAST Insulating Refractory Castable

CPYRO152 / 1873

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.