MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
P & P Technology BeCu alloy 25 (CA172) Contact Finger Strips
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: The CFS range of contact finger strips are available in Beryllium Copper, Phosphor Bronze and Stainless Steel. Many plating options are also available. Contact finger strips are used to close the aperture between two surfaces and provide high EMI shielding effectiveness. The strips are very versatile in applications where low closure force is required such as enclosures.

Material Specification: (Beryllium Copper) BeCu alloy 25(CA172) is used for maximum spring, strength and fatigue resistance.

Information provided by P & P Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 175 - 185 MPaHeat Treated
Modulus of Elasticity 185 GPaHeat Treated
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.00000769 - 0.0000080 ohm-cmHeat Treated
Shielding Effectiveness >= 110 dB
@Frequency 100000 Hz
H-Field
 >= 110 dB
@Frequency 1e+7 Hz
E-Field
 >= 110 dB
@Frequency 1e+9 Hz
P-Field
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 1.8 - 2.0 %
Co + Ni >= 0.20 %
Co + Ni + Fe >= 0.60 %
Copper, Cu 97.2 %
 
Descriptive Properties
Temper1000 psiHeat Treated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Brush Wellman Beryllium-Copper Alloy 171 1/2 HT (TH02) Temper
Ampco Metal AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, >50.8 mm.
Brush Wellman Beryllium Copper Alloy 10 Strip; HTC Temper (UNS C17500)
Brush Wellman Beryllium Copper Alloy 165 Strip; 1/2H (TD02) Temper (UNS C17000)

PPPTEC005 / 133469

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.