MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Brush Wellman Beryllium Copper Alloy 165 Strip; 1/2H (TD02) Temper (UNS C17000)  (discontinued **)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Treatment required for max strength: as supplied
Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.5
Formability Ratio (bad Way): 1
Superficial Hardness: 30T 74-79

Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: ASTM B-194, QQ-C-533
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.41 g/cc0.304 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 88 - 9688 - 96
Hardness, Vickers 176 - 216176 - 216
Tensile Strength, Ultimate 580 - 690 MPa84100 - 100000 psi
Tensile Strength, Yield 510 - 660 MPa74000 - 95700 psi
Elongation at Break 12 - 30 %12 - 30 %
Modulus of Elasticity 131 GPa19000 ksi
Fatigue Strength 220 - 260 MPa
@# of Cycles 1.00e+8
31900 - 37700 psi
@# of Cycles 1.00e+8
Reverse Bending (R=1)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000910 - 0.0000115 ohm-cm0.00000910 - 0.0000115 ohm-cm15-19% IACS Conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
9.44 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 105 W/m-K729 BTU-in/hr-ft²-°F
Melting Point 870 - 980 °C1600 - 1800 °F
Solidus 870 °C1600 °F
Liquidus 980 °C1800 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 1.6 - 1.79 %1.6 - 1.79 %
Co + Ni >= 0.20 %>= 0.20 %
Co + Ni + Fe <= 0.60 %<= 0.60 %
Copper, Cu 98 %98 %as balance

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Brush Wellman Beryllium-Copper Alloy 171 1/2 HT (TH02) Temper
Brush Wellman Beryllium-Copper Alloy 171 1/4 HT (TH01) Temper
Materion Alloy 10X CuCoBeZr Alloy, TH04 Temper
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; A (TB00) Temper (UNS C17500)
Materion Beryllium Copper Alloy 10 Forgings & Extrusions; AT (TF00) Temper (UNS C17500)

NBB444 / 15175

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.