MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Brush Wellman Beryllium Copper Alloy 10 Strip; HTC Temper (UNS C17500)  (discontinued **)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: Treatment required for max strength: Mill Hardened
Stress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 94%
Stress Relaxation after 1000 hrs @ 200°C: 72%
Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 1
Formability Ratio (bad Way): 1
Superficial Hardness: 30T 69-75

Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.

Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.

Key Words: ASTM B-534, RWMA Class 3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 79 - 8879 - 88
Hardness, Vickers 147 - 176147 - 176
Tensile Strength, Ultimate 510 - 590 MPa74000 - 85600 psi
Tensile Strength, Yield 340 - 520 MPa49300 - 75400 psi
Elongation at Break 8.0 - 20 %8.0 - 20 %
Modulus of Elasticity 138 GPa20000 ksi
Fatigue Strength 210 - 240 MPa
@# of Cycles 1.00e+8
30500 - 34800 psi
@# of Cycles 1.00e+8
Reverse Bending (R=1)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity <= 0.00000290 ohm-cm<= 0.00000290 ohm-cm>60% IACS conductivity
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 200 °C
10.0 µin/in-°F
@Temperature 68.0 - 392 °F
Thermal Conductivity 200 W/m-K1390 BTU-in/hr-ft²-°F
Melting Point 1010 - 1050 °C1850 - 1920 °F
Solidus 1010 °C1850 °F
Liquidus 1050 °C1920 °F
 
Component Elements PropertiesMetricEnglishComments
Beryllium, Be 0.40 - 0.70 %0.40 - 0.70 %
Cobalt, Co 2.4 - 2.7 %2.4 - 2.7 %
Copper, Cu 97 %97 %as balance

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ampco Metal AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, >50.8 mm.
Ampco Metal AMPCOLOY® 95 Cobalt-Copper Alloy, Extrusion, < 50.8 mm.
Materion Beryllium Copper Alloy 10 Plate & Rolled Bar; H (TD04) Temper; up to 76 mm Thickness (UNS C17500)
Materion Beryllium Copper Alloy 10 Rod and Bar; HT (TH04) Temper; up to 76 mm (UNS C17500)
Materion Beryllium Copper Alloy 10 Wire; HT (TH04) Temper; 1.3-12.7 mm Diameter (UNS C17500)

NBB388 / 15147

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.