MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total XT10B High Density Polyethylene, Pipe Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Polyethylene: HDPE Bimodal PE4710 pipe resin (Black)

Characteristics:

  • Outstanding high temperature creep rupture strength
  • Outstanding slow crack growth resistance
  • Excellent resistance to rapid crack propagation
  • NSF certified to D2513 (gas), CSA B137.4 (gas), CSA B137.1 (water) and CSA C448 (geothermal)
  • NSF Standard 14/61 Certified

Applications:

  • Gas distribution
  • Potable water
  • Molded fittings
  • Industrial & mining
  • Gas and oil gathering
  • General pipe relining

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.958 g/ccASTM D792
Carbon Black Loading 2.5 %ASTM D1603
Melt Flow 0.20 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 7.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 1000 hourASTM F1473
Tensile Strength, Yield 3600 psiASTM D638
Elongation at Break >= 500 %ASTM D638
Flexural Modulus 160000 psi
@Strain 1 %
ASTM D790
Hydrostatic Design Basis 1000 psi
@Temperature 60.0 °C
ASTM D2837
 1600 psi
@Temperature 22.8 °C
ASTM D2837
 
Thermal PropertiesOriginal ValueComments
Melting Point 266 - 270 °FASTM D3417
 
Descriptive Properties
Cell Classification445574C, 445576CASTM D3350
Minimum Required Strength10 MPaISO 9080/ISO 12162
Pipe Test CategoryCECASTM D2513

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil HD 6480.UV High Density Polyethylene Resin
Total XT25N High Density Polyethylene, Pipe Resin
Borealis BorSafe™ HE3494-LS-H HDPE Compound for Pressure Pipes
Total XT10 N High Density Polyethylene - Pipe Resin
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes

PTOTAL752 / 130477

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.