MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total XT25N High Density Polyethylene, Pipe Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Polyethylene: High molecular weight, bimodal pipe resin. PPI TR4 designation PE4710 /PE100 for demanding installations. Every batch certified to meet 2500 hrs PENT according to ASTM F1473.

Characteristics:

  • Outstanding high temperature creep rupture strength
  • Exceptional slow crack growth resistance certified as exceeding 2500 hrs PENT
  • Excellent resistance to rapid crack propagation
  • NSF certified to D2513 (gas), CSA B137.4 (gas), CSA B137.1 (water) and CSA C448 (geothermal)
  • NSF Standard 14/61 Certified
  • FDA Compliant

Applications:

  • Gas distribution
  • Potable water
  • Geothermal
  • Industrial mining
  • Sewer and sewer relining
  • Gas and oil gathering
  • General pipe relining
  • Pipe coating

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.949 g/cc0.949 g/ccASTM D792
Melt Flow 7.5 g/10 min
@Load 21.6 kg,
Temperature 190 °C
7.5 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
PENT >= 2500 hour>= 2500 hourASTM F1473
Tensile Strength, Yield >= 24.1 MPa>= 3500 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus 1.03 GPa
@Strain 2 %
150 ksi
@Strain 2 %
ASTM D790
Izod Impact, Notched 4.27 J/cm
@Thickness 3.17 mm
8.00 ft-lb/in
@Thickness 0.125 in
ASTM D256
Hydrostatic Design Basis  6.89 MPa
@Temperature 60.0 °C
1000 psi
@Temperature 140 °F
ASTM D2837
 11.0 MPa
@Temperature 22.8 °C
1600 psi
@Temperature 73.0 °F
ASTM D2837
 
Thermal PropertiesMetricEnglishComments
Melting Point 131 °C268 °FASTM D3417
Heat Distortion Temperature 77.8 °C172 °FASTM D648
Brittleness Temperature -118 °C-180 °FASTM D746
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Cell Classification445574, 445576ASTM D3350
Minimum Required Strength10 MPaISO 9080
Notched Pipe Test>500 hrsISO 13479
Pipe Test CategoryCECASTM D2239
Resistance to Rapid Crack Propagation>12 barISO 13477, S4, Critical Pressure, 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total XT10B High Density Polyethylene, Pipe Resin
Total XLS 12 B High Density Polyethylene - Pipes and Fittings
ExxonMobil HD 6480.UV High Density Polyethylene Resin
Borealis BorSafe™ HE3494-LS-H HDPE Compound for Pressure Pipes
Total XSene® XRC 20 B High Density Polyethylene - Pipes and Fittings

PTOTAL750 / 130475

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.