Product Description: ExxonMobil™ HD 6480.UV is a UV stabilized HDPE grade, characterized by excellent dimensional stability, very high stiffness and good impact strength. Availability: Africa & Middle East, Asia Pacific and Europe Additive: - Thermal Stabilizer: Yes
- UV Stabilizer: Yes
Applications: - Industrial Pails
- Vegetable and Bottle Crates
Information provided by ExxonMobil |