MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2020509D1 Copper Ink  (discontinued **)
Categories: Fluid; Metal; Electronic/Magnetic Alloy; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: C2020509D1 is designed for BME End Terminations. The ink is designed for application using a Palomer dipping system. It can be used for Chipstar dippers, but the rheology needs of the customer have to be defined. It has excellent cosmetics and fires to a dense, smooth termination with high bond strength. It is designed to be used with standard Nickel/Tin Plating Systems.

This Ink has been made at a ready to use viscosity and should be gently stirred before use avoiding introduction of air bubbles.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.00 g/cc
Solids Content 74 - 76 %
Viscosity 10400 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT550 cone and plate viscometer with the PK1.1°
Brookfield Viscosity 33125 cP
@Temperature 25.0 °C
10 rpm
Storage Temperature 20.0 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 150 °C
Dry Time 0.25 hourwith air flow
 
Descriptive Properties
CosmeticsExcellent
PlateabilityExcellent
SolderabilityExcellent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
FloMet Fe-3% Si Soft Magnetic Alloy
FloMet ASTM F-15 Controlled Thermal Expansivity Alloy
FloMet 430L Stainless Steel
FloMet Permalloy® 4-79 Moly Soft Magnetic Alloy
FloMet Fe-50%Co Soft Magnetic Alloy

WGEM007 / 75860

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.