MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

FloMet Fe-50%Co Soft Magnetic Alloy
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: FloMet provides precision miniature components through metal injection molding (MIM). Metal powders are mixed with thermoplastic binders to form a homogeneous mixture, with approximately 60% volume metal powder and 40% volume plastic. The mixture (referred to as feedstock) is then injection molded at relatively low temperatures and pressures in conventional plastic injection molding machines. The molded green parts are then thermally processed in two steps. First, the binder is removed by evaporation in an operation called debinding. Next, the part is sintered in a dry hydrogen atmosphere, which densifies the part isotropically. The complex shape of the original molded part is retained throughout the process, and close tolerances can be achieved. Density is typically 95-98% of the wrought metal; mechanical properties and corrosion resistance are similar to wrought material

Information provided by FloMet LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 8080
Tensile Strength, Ultimate 207 MPa30000 psi
Tensile Strength, Yield 207 MPa
@Strain 0.2 %
30000 psi
@Strain 0.2 %
Elongation at Break <= 1.0 %<= 1.0 %
 
Electrical PropertiesMetricEnglishComments
Magnetic Permeability <= 4900<= 4900µmax in G/Oe with a magnetizing field of 25 Oe.
Magnetic Coercive Force, Hc 1.9 Oe1.9 Oe
Magnetic Saturation Flux Density, Bmax 18900 Gauss18900 GaussMagnetizing field of 25 Oe.
 21100 Gauss21100 GaussMagnetizing field of 500 Oe.
Magnetic Remanence, Br 14400 Gauss14400 GaussMagnetizing field of 25 Oe.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.050 %<= 0.050 %
Cobalt, Co 50 %50 %
Iron, Fe 50 %50 %As remainder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
FloMet Fe-3% Si Soft Magnetic Alloy
FloMet Permalloy® 4-79 Moly Soft Magnetic Alloy
Carpenter Hiperco® Alloy 50 Fe-Co-V Soft Magnetic Alloy, Cold Rolled
FloMet 430L Stainless Steel
FloMet ASTM F-15 Controlled Thermal Expansivity Alloy

NXFLOM05 / 20016

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.