MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Titanium Ti-6Al-2Sn-4Zr-2Mo (Ti-6-2-4-2), Sheet
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: Unspecified heat treatment. Alpha Alloy. Silicon is often added to improve creep resistance (See Ti-6242S).

Characteristics: Good elevated-temperature performance, good creep strength

Applications: High-temp jet engines. Blades, discs, spacers, seals. High performance automotive valves.

1 other heat treatment of this alloy is in MatWeb.

Key Words: Ti6Al2Sn4Zr2Mo, Ti-6242; Ti-6-2-4-2; UNS R54620
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.54 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 318Estimated from Rockwell C.
Hardness, Knoop 346Estimated from Rockwell C.
Hardness, Rockwell C 34Estimated from similar materials
Hardness, Vickers 333Estimated from Rockwell C.
Tensile Strength 710 MPa
@Temperature 540 °C
 830 MPa
@Temperature 371 °C
 890 MPa
@Temperature 204 °C
Tensile Strength, Ultimate 1010 MPa
Tensile Strength, Yield 990 MPa
 570 MPa
@Temperature 540 °C
0.2% offset
 650 MPa
@Temperature 371 °C
0.2% offset
 760 MPa
@Temperature 204 °C
0.2% offset
Elongation at Break 3.0 %
 10.8 %
@Temperature 204 °C
 11.5 %
@Temperature 371 °C
 17.8 %
@Temperature 540 °C
Tensile Modulus 120 GPa
Compressive Yield Strength 1080 MPa0.2 % Permanent Set
 635 MPa
@Temperature 540 °C
0.2% offset
 695 MPa
@Temperature 371 °C
0.2% offset
 800 MPa
@Temperature 204 °C
0.2% offset
Compressive Modulus 130 GPa
Poissons Ratio 0.32duplex annealed
Fracture Toughness 148 MPa-m½Plane-Strain
Shear Modulus 45.5 GPaCalculated
Shear Strength 690 MPaUltimate shear strength
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000190 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.70 µm/m-°C
@Temperature 20.0 - 100 °C
 8.10 µm/m-°C
@Temperature 20.0 - 315 °C
average
 8.10 µm/m-°C
@Temperature 20.0 - 540 °C
average
Specific Heat Capacity 0.460 J/g-°C
Thermal Conductivity 7.10 W/m-K
Melting Point <= 1700 °CEstimated from similar materials
Liquidus 1700 °CEstimated from similar materials
Beta Transus 990 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 6.0 %
Carbon, C <= 0.050 %
Hydrogen, H <= 0.0125 %
Iron, Fe <= 0.25 %
Molybdenum, Mo 2.0 %
Nitrogen, N <= 0.050 %
Other, each <= 0.10 %
Other, total <= 0.30 %
Oxygen, O <= 0.12 %
Titanium, Ti 88 %
Zirconium, Zr 4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Ti-6Al-2Sn-4Zr-2Mo (Ti-6-2-4-2), Duplex Annealed
Titanium Ti-6Al-2Sn-4Zr-2Mo-0.1Si; Duplex Annealed
Titanium Ti-6Al-4V (Grade 5), Annealed
Alcoa Deltalloy® 4032-T86 Aluminum
Titanium Ti-8Al-1Mo-1V (Ti-8-1-1) Annealed 8 hr at 790°C (1450°F)

MTA642 / 14133

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.