MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Alcoa Deltalloy® 4032-T86 Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 4000 Series Aluminum Alloy

Material Notes: Weldability = B; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = C (A = best; E = worst). General 4032 characteristics and uses: Good machinability and drilling characteristics when using single point or multi-spindle screw machines. Excellent surface finish using polycrystalline or carbide tooling. Superior wear resistance, eliminated the need for hard coat anodizing. High strength, low thermal expansion.

Uses: Master brake cylinders, transmission valves, copier parts, bushings for rack and pinion steering systems, sound recording devices, bearings and hydraulic applications, forged pistons.

Data supplied by the manufacturer, Alcoa.

Key Words: Aluminum 4032-T86; 4032-T86 Aluminium; UNS A94032; Alcoa, Aluminum Company of America; AA4032-T86
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.68 g/cc0.0968 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 120120500 kg load/10 mm ball
Hardness, Knoop 150150Estimated from Brinell
Hardness, Rockwell A 46.846.8Estimated from Brinell
Hardness, Rockwell B 7575Estimated from Brinell
Hardness, Vickers 136136Estimated from Brinell
Tensile Strength, Ultimate >= 365 MPa>= 52900 psi
Tensile Strength, Yield >= 338 MPa>= 49000 psi
Elongation at Break 5.0 %5.0 %
Modulus of Elasticity 79.0 GPa11500 ksi
Machinability 70 %70 %0-100 Scale (A=90; B=70; C=50; D=30; E=10)
Shear Strength 218 MPa31600 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000490 ohm-cm0.00000490 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 19.4 µm/m-°C
@Temperature 20.0 - 100 °C
10.8 µin/in-°F
@Temperature 68.0 - 212 °F
average
Thermal Conductivity 138 W/m-K958 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 85 %85 %
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 0.50 - 1.3 %0.50 - 1.3 %
Iron, Fe <= 1.0 %<= 1.0 %
Magnesium, Mg 0.80 - 1.3 %0.80 - 1.3 %
Nickel, Ni 0.50 - 1.3 %0.50 - 1.3 %
Silicon, Si 11 - 13.5 %11 - 13.5 %
Zinc, Zn <= 0.25 %<= 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alcoa Deltalloy® 4032-T651 Aluminum
Aluminum 4032-T6
Aluminum 4032-O
Aluminum 2099 Composition Spec
Titanium Ti-6Al-2Sn-4Zr-2Mo (Ti-6-2-4-2), Sheet

NALCOA01 / 14744

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.