MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

LG Chemical HIPS 408AF Injection Molding Grade
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Flame Retardant

Applications: Electric Parts Requiring Flame Retardancy

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0080 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 6.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
6.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238(I)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9494ASTM D785
Tensile Strength, Yield 26.5 MPa
@Thickness 3.20 mm
3840 psi
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Break 60 %
@Thickness 3.20 mm
60 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Elongation at Yield >= 5.0 %
@Thickness 3.20 mm
>= 5.0 %
@Thickness 0.126 in
50 mm/min; ASTM D638
Flexural Strength 39.2 MPa
@Thickness 3.20 mm
5690 psi
@Thickness 0.126 in
15 mm/min; ASTM D790
Flexural Modulus 2.16 GPa
@Thickness 3.20 mm
313 ksi
@Thickness 0.126 in
15 mm/min; ASTM D790
Izod Impact, Notched  0.392 J/cm
@Thickness 6.40 mm,
Temperature -30.0 °C
0.735 ft-lb/in
@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
 0.490 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
0.918 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 0.883 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
1.65 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 1.27 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
2.39 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
@Thickness 6.40 mm
189 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
@Thickness 6.40 mm
178 °F
@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 84.0 °C
@Load 5.00 kg
183 °F
@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical 50.0 °C122 °FUL 746B
UL RTI, Mechanical with Impact 50.0 °C122 °FUL 746B
UL RTI, Mechanical without Impact 50.0 °C122 °FUL 746B
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 200 °C356 - 392 °F
Middle Barrel Temperature 190 - 200 °C374 - 392 °F
Front Barrel Temperature 200 - 210 °C392 - 410 °F
Nozzle Temperature 200 - 230 °C392 - 446 °F
Melt Temperature 200 - 230 °C392 - 446 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 60.0 - 70.0 °C
@Time 10800 - 14400 sec
140 - 158 °F
@Time 3.00 - 4.00 hour
Moisture Content >= 0.010 %>= 0.010 %
Back Pressure 29.4 - 58.8 MPa4260 - 8530 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical HIPS 403AF PS, Flame Retardant
Overview of materials for Nylon 6, Impact Grade
LG Chemical 65IH HIPS
LG Chemical 60HR-G HIPS
LG Chemical 60HR HIPS

PLHCHEM9978 / 239494

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.