MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical 65IH HIPS  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food trays, and disposable food containers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm0.0040 - 0.0080 in/inASTM D955
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9797ASTM D785
Tensile Strength, Yield 29.5 MPa4280 psi50 mm/min; ASTM D638
Elongation at Break 60 %60 %50 mm/min; ASTM D638
Flexural Yield Strength 47.1 MPa6830 psi15 mm/min; ASTM D790
Flexural Modulus 2.10 GPa305 ksi15 mm/min; ASTM D790
Izod Impact, Notched  0.930 J/cm
@Thickness 6.35 mm
1.74 ft-lb/in
@Thickness 0.250 in
ASTM D256
 1.37 J/cm
@Thickness 3.17 mm
2.57 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 400 - 600 V400 - 600 VUL Rating PLC 1 (400-600 volts)
Hot Wire Ignition, HWI 15 - 30 sec15 - 30 secUL Rating PLC 3 (15-30 sec)
High Amp Arc Ignition, HAI >= 120 arcs>= 120 arcsUL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR <= 10.0 mm/min<= 0.394 in/minUL Rating PLC 0 (0-10 mm/min)
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
@Thickness 12.7 mm
172 °F
@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 99.0 °C210 °F1000 g; ASTM D1525
Flammability, UL94  HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in
 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Flame Spread 30.0 mm/min
@Thickness 3.17 mm
1.18 in/min
@Thickness 0.125 in
FH3
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical 501S-S HIPS
LG Chemical 60HR HIPS
LG Chemical 60HR-G HIPS
Total Lacqrene® 4241 High Impact Polystyrene
LG Chemical 25SPR GPPS

PLAZ86 / 50344

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.