MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

BASF Pluracol® 945 Molded Foam Polyol
Categories: Fluid

Material Notes: Description: Pluracol® 945 polyol is a high molecular weight polyol for use in high water, low-density automotive seating foams where a high degree of foam stability is required. In combination with graft polyols, such as Pluracol 973, Pluracol 945 produces molded foams from high-water, low-density formulations. These foams are less susceptible to mold leakage, voiding and basal cells than foams produced with other polyols, but do require crushing to prevent shrinkage. Pluracol 945 is more reactive than either Pluracol 816 or Pluracol 538.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.00 g/cc
@Temperature 48.9 °C
0.0361 lb/in³
@Temperature 120 °F
 1.01 g/cc
@Temperature 37.8 °C
0.0365 lb/in³
@Temperature 100 °F
 1.02 g/cc
@Temperature 25.0 °C
0.0368 lb/in³
@Temperature 77.0 °F
Viscosity  270 cP
@Temperature 48.9 °C
270 cP
@Temperature 120 °F
 370 cP
@Temperature 37.8 °C
370 cP
@Temperature 100 °F
 850 cP
@Temperature 25.0 °C
850 cP
@Temperature 77.0 °F
 
Chemical PropertiesMetricEnglishComments
Total Acid Number <= 0.010<= 0.010STI 3063/3161
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.16 J/g-°C0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K0.868 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %STI 3062
 
Descriptive Properties
Color<30APHA, STI 3057
 Clear Liquid
CompositionNa & K<5 ppm, STI 3038
Hydroxyl Number34 - 36 mg KOH/gSTI 3007/3162
Unsaturation<0.05 meq/gSTI 3056

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Pluracol® 922 Rigid Polyol
BASF Pluracol® 858 Specialty Polyol
BASF Pluracol® 736 Rigid Polyol
BASF Pluracol® 735 Rigid Polyol
BASF Pluracol® 1026 Molded Foam Polyol

PBASG0803 / 132436

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.