MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Pluracol® 736 Rigid Polyol
Categories: Fluid

Material Notes: Description: Pluracol® 736 polyol is an aromatic initiator-based polyol which can be used in a variety of rigid foam formulations. This polyol can be reacted with crude MDI, crude TDI or TDI quasiprepolymers. Formulations containing Pluracol 736 can be utilized for foaming building and door panels, refrigerators and freezers, and other insulating products such as portable ice chests and water coolers. Pluracol 736 has good compatibility with common foam ingredients and improves the processability of low density foam formulations. Pluracol 736 is not recommended for use in quasi-prepolymer preparations.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  1.01 g/cc
@Temperature 70.0 °C
0.0365 lb/in³
@Temperature 158 °F
 1.03 g/cc
@Temperature 60.0 °C
0.0372 lb/in³
@Temperature 140 °F
 1.04 g/cc
@Temperature 40.0 °C
0.0376 lb/in³
@Temperature 104 °F
Viscosity  400 cP
@Temperature 60.0 °C
400 cP
@Temperature 140 °F
 415 cP
@Temperature 70.0 °C
415 cP
@Temperature 158 °F
 14500 cP
@Temperature 40.0 °C
14500 cP
@Temperature 104 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %STI 3062
 
Descriptive Properties
ColorBrown Liquid
Hydroxyl Number380 - 400 mg KOH/gSTI 3007/3162

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Pluracol® 735 Rigid Polyol
BASF Pluracol® 922 Rigid Polyol
Covestro Bayfit® Low Density Polyurethane Flexible Molded Foam,
BCC Products MB 1300 Polyurethane Foam Modeling Board
BCC Products MB 1150 Polyurethane Foam Modeling Board

PBASG0798 / 132431

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.