MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Pluracol® 858 Specialty Polyol
Categories: Fluid

Material Notes: Description: Pluracol® 858 polyol is a modifying polyol which can be used in a wide variety of applications. It can be employed as a cross-linking agent for rigid foam as well as coatings and elastomers. When combined with GP series polyols, high heat distortion resistant microcellular products can be produced.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.986 g/cc
@Temperature 43.4 °C
0.0356 lb/in³
@Temperature 110 °F
 0.996 g/cc
@Temperature 32.2 °C
0.0360 lb/in³
@Temperature 90.0 °F
 1.00 g/cc
@Temperature 25.0 °C
0.0361 lb/in³
@Temperature 77.0 °F
Viscosity  285 cP
@Temperature 43.4 °C
285 cP
@Temperature 110 °F
 700 cP
@Temperature 32.2 °C
700 cP
@Temperature 90.0 °F
 1360 cP
@Temperature 25.0 °C
1360 cP
@Temperature 77.0 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.050 %<= 0.050 %STI 3062
 
Descriptive Properties
ColorClear Liquid
Hydroxyl Number935 mg KOH/gSTI 3007/3162

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Pluracol® 922 Rigid Polyol
BASF Pluracol® 593 Specialty Polyol
BASF Pluracol® GP 730 Specialty Polyol
Indorama AlphaPet Preformance® 1708CC(A) PET Resin
BASF Pluracol® 735 Rigid Polyol

PBASG0800 / 132433

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.