MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
430 Stainless Steel annealed and cold drawn bar, 25 mm diameter
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes:

Key Words: UNS S43000, AMS 5503, AMS 5627, ASME SA182, ASME SA240, ASME SA268, ASME SA479, ASTM A176, ASTM A182, ASTM A240, ASTM A268, ASTM A276, ASTM A314, ASTM A473, ASTM A479, ASTM A493, ASTM A511, ASTM A554, ASTM A580, ASTM A651, B.S. 430 S 15, ferritic, DIN 1.4016, AFNOR Z 8 C 17 (Fr), UNI X 8 Cr 17, JIS SUS 430, SS14 2320 (Sweden), FED QQ-S-763, FED QQ-S-766, FED STD-66, MIL SPEC MIL-S-862, SAE J405 (51430), ISO 683/13 8
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 7.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 185
Hardness, Knoop 206Converted from Brinell
Hardness, Rockwell B 90Converted from Brinell
Hardness, Vickers 194Converted from Brinell
Tensile Strength, Ultimate 586 MPa
Tensile Strength, Yield 483 MPa
@Strain 0.2 %
Elongation at Break 20 %in 50 mm
Modulus of Elasticity 200 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000600 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 600 - 1100annealed condition at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.4 µm/m-°C
@Temperature 0.000 - 100 °C
 11.0 µm/m-°C
@Temperature 0.000 - 315 °C
 11.3 µm/m-°C
@Temperature 0.000 - 540 °C
 11.9 µm/m-°C
@Temperature 0.000 - 650 °C
 12.4 µm/m-°C
@Temperature 0.000 - 815 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 26.1 W/m-K
@Temperature 100 °C
 26.3 W/m-K
@Temperature 500 °C
Melting Point 1425 - 1510 °C
Solidus 1425 °C
Liquidus 1510 °C
Maximum Service Temperature, Air 815 °CContinuous Service
 870 °CIntermittent
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.12 %
Chromium, Cr 14 - 18 %
Iron, Fe 79 - 87 %As Remainder
Manganese, Mn <= 1.0 %
Phosphorus, P <= 0.040 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
430 Stainless Steel annealed bar
AISI Type 430F Stainless Steel
AISI Type 430F Stainless Steel annealed and cold drawn bar 25 mm diameter
AISI Type 430F Stainless Steel annealed bar
430 Stainless Steel annealed sheet

MQ430AT / 13128

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.