MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

430 Stainless Steel annealed and cold drawn bar, 25 mm diameter
Categories: Metal; Ferrous Metal; Stainless Steel; T 400 Series Stainless Steel

Material Notes:

Key Words: UNS S43000, AMS 5503, AMS 5627, ASME SA182, ASME SA240, ASME SA268, ASME SA479, ASTM A176, ASTM A182, ASTM A240, ASTM A268, ASTM A276, ASTM A314, ASTM A473, ASTM A479, ASTM A493, ASTM A511, ASTM A554, ASTM A580, ASTM A651, B.S. 430 S 15, ferritic, DIN 1.4016, AFNOR Z 8 C 17 (Fr), UNI X 8 Cr 17, JIS SUS 430, SS14 2320 (Sweden), FED QQ-S-763, FED QQ-S-766, FED STD-66, MIL SPEC MIL-S-862, SAE J405 (51430), ISO 683/13 8
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 185185
Hardness, Knoop 206206Converted from Brinell
Hardness, Rockwell B 9090Converted from Brinell
Hardness, Vickers 194194Converted from Brinell
Tensile Strength, Ultimate 586 MPa85000 psi
Tensile Strength, Yield 483 MPa
@Strain 0.2 %
70100 psi
@Strain 0.2 %
Elongation at Break 20 %20 %in 50 mm
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000600 ohm-cm
@Temperature 20.0 °C
0.0000600 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 600 - 1100600 - 1100annealed condition at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.4 µm/m-°C
@Temperature 0.000 - 100 °C
5.78 µin/in-°F
@Temperature 32.0 - 212 °F
 11.0 µm/m-°C
@Temperature 0.000 - 315 °C
6.11 µin/in-°F
@Temperature 32.0 - 599 °F
 11.3 µm/m-°C
@Temperature 0.000 - 540 °C
6.28 µin/in-°F
@Temperature 32.0 - 1000 °F
 11.9 µm/m-°C
@Temperature 0.000 - 650 °C
6.61 µin/in-°F
@Temperature 32.0 - 1200 °F
 12.4 µm/m-°C
@Temperature 0.000 - 815 °C
6.89 µin/in-°F
@Temperature 32.0 - 1500 °F
Specific Heat Capacity 0.460 J/g-°C
@Temperature 0.000 - 100 °C
0.110 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  26.1 W/m-K
@Temperature 100 °C
181 BTU-in/hr-ft²-°F
@Temperature 212 °F
 26.3 W/m-K
@Temperature 500 °C
183 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1425 - 1510 °C2597 - 2750 °F
Solidus 1425 °C2597 °F
Liquidus 1510 °C2750 °F
Maximum Service Temperature, Air 815 °C1500 °FContinuous Service
 870 °C1600 °FIntermittent
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Chromium, Cr 14 - 18 %14 - 18 %
Iron, Fe 79 - 87 %79 - 87 %As Remainder
Manganese, Mn <= 1.0 %<= 1.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
430 Stainless Steel annealed bar
AISI Type 430F Stainless Steel
AISI Type 430F Stainless Steel annealed and cold drawn bar 25 mm diameter
AISI Type 430F Stainless Steel annealed bar
430 Stainless Steel annealed sheet

MQ430AT / 13128

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.