MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik SAF 2205 for wirelines Wire
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sandvik SAF 2205 is a duplex (austenitic/ferritic) stainless steel suitable for service in corrosive oil and gas wells. The grade is characterized by:
  • High resistance to stress corrosion cracking (SCC) in chloride and CO containing environments
  • High resistance to pitting owing to its high PRE* value of 35 minimum
  • High resistance to general corrosion
  • High tensile strength
Sandvik SAF 2205 is suitable for service in wells with a H S partial pressure of max. 3 psi. Service temperature: 50 to 280°C (60 to 540°F)

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate >= 1700 MPa>= 247000 psi
Tensile Strength, Yield >= 1530 MPa
@Strain 0.2 %
>= 222000 psi
@Strain 0.2 %
Modulus of Elasticity 200 GPa29000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.0000740 ohm-cm
@Temperature 20.0 °C
0.0000740 ohm-cm
@Temperature 68.0 °F
 0.0000850 ohm-cm
@Temperature 100 °C
0.0000850 ohm-cm
@Temperature 212 °F
 0.0000960 ohm-cm
@Temperature 200 °C
0.0000960 ohm-cm
@Temperature 392 °F
 0.000100 ohm-cm
@Temperature 300 °C
0.000100 ohm-cm
@Temperature 572 °F
 0.000110 ohm-cm
@Temperature 400 °C
0.000110 ohm-cm
@Temperature 752 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 280 °C536 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.030 %<= 0.030 %
Chromium, Cr 22 %22 %
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo 3.2 %3.2 %
Nickel, Ni 5.5 %5.5 %
Nitrogen, N 0.18 %0.18 %
Phosphorus, P <= 0.030 %<= 0.030 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.015 %<= 0.015 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AK Steel 2205 Duplex Stainless steel
Indium Corp. 2205 Rosin Flux
Carlson 2205 (UNS S32205) Duplex Stainless Steel
Sandvik SAF 2205 Hollow Bar
Sandvik SAF 2205 Billet

NSANDV5224 / 199788

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.