MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Indium Corp. 2205 Rosin Flux
Categories: Fluid

Material Notes: 2205 is an alcohol-based flux that is ideal for soldering all surface finishes. It can be used to test solderability according to IPC J-STD-003 and IPC J-STD-002.

Features

  • Meets J-STD-003/2 specifications for flux type 1
  • Non-corrosive residue

Physical Properties

  • Color: Amber
  • Flux Type: ROL1

Information Provided by Indium Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity  0.843 g/cc
@Temperature 25.0 °C
0.843 g/cc
@Temperature 77.0 °F
 0.848 g/cc
@Temperature 15.5 °C
0.848 g/cc
@Temperature 59.9 °F
Solids Content 26.4 %26.4 %
 
Chemical PropertiesMetricEnglishComments
Acid Value 17.1517.15
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance  5.36e+9 ohm
@Time 346000 sec
5.36e+9 ohm
@Time 96.0 hour
Control; IPC B24
 1.23e+10 ohm
@Time 86400 sec
1.23e+10 ohm
@Time 24.0 hour
Control; IPC B24
 
Thermal PropertiesMetricEnglishComments
Flash Point 12.0 °C53.6 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Outokumpu 2205 Duplex Stainless Steel
AK Steel 2205 Duplex Stainless steel
Carlson 2205 (UNS S32205) Duplex Stainless Steel
Carlson 2205 (UNS S31803) Duplex Stainless Steel
MetalTek MTEK 2205 Cast UNS J92205 Duplex Stainless Steel

NNIN972 / 131611

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.