MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company PermaStat® 100 UV Polypropylene (PP); ESD Protection - Permanently Anti-static - UV Stabilized
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: This compound has been formulated to meet the following surface resistance requirement of IEC 60079-0: <1E11 ohm at 30% RH.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.920 g/cc0.920 g/ccASTM D 792
Linear Mold Shrinkage 0.010 - 0.015 cm/cm
@Thickness 3.20 mm
0.010 - 0.015 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 29.6 MPa4300 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 1.45 GPa210 ksiASTM D 638
Flexural Strength 44.8 MPa6500 psiASTM D 790
Flexural Modulus 1.52 GPa220 ksiASTM D 790
Izod Impact, Notched 0.534 J/cm
@Thickness 3.20 mm
1.00 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 - 9.90e+10 ohm-cm1.00e+9 - 9.90e+10 ohm-cmASTM D 257
Surface Resistivity per Square 1.00e+10 - 9.90e+11 ohm1.00e+10 - 9.90e+11 ohmASTM D 257; ESD STM11.11
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Processing PropertiesMetricEnglishComments
Melt Temperature 171 - 204 °C340 - 400 °F
Mold Temperature 32.2 - 65.6 °C90.0 - 150 °F
Drying Temperature 79.4 °C
@Time 7200 sec
175 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Injection Pressure 48.3 - 75.8 MPa7000 - 11000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Covestro Makrolon® 2405 MAS048 Polycarbonate
Celanese VECTRA A950 LCP, Unfilled
Celanese VECTRA A515 LCP, 15% Mineral Reinforced
Avient Edgetek® CY-1000 UV FR V0 Acrylonitrile Butadiene Styrene + PC (ABS+PC)

PQZRA38710 / 206087

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.