MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® CY-1000 UV FR V0 Acrylonitrile Butadiene Styrene + PC (ABS+PC)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate (PC)

Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Water Absorption 0.10 %0.10 %@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 58.6 MPa8500 psiASTM D638
Elongation at Break 10 %10 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.14 GPa310 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 96.5 MPa14000 psiASTM D790
Flexural Modulus 2.62 GPa380 ksiASTM D790
Izod Impact, Notched 1.10 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
2.06 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D257
Surface Resistance 1.00e+14 ohm1.00e+14 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 65.6 °C150 °FUnannealed; ASTM D648
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0626 in
ALL; Internal Method
 
Descriptive Properties
FeaturesFlame Retardant
FormsPellets
Generic MaterialABS+PC
Generic NameAcrylonitrile Butadiene Styrene + PC (ABS+PC)
Outdoor Suitabilityf2UL 746C
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
304 Stainless Steel
Bhansali Engineering Abstron IMC-45 ABS-PC Alloy
LyondellBasell Pro-fax SG702 Polypropylene Impact Copolymer
A. Schulman Diamond ABS/PC FC-30
A. Schulman Diamond ABS/PC 7901

PH0POL0785 / 145354

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.