MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese VECTRA A950 LCP, Unfilled
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Unreinforced Vectra grade suitable for extrusion.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ISO 1183
Moisture Absorption 0.00300 %0.00300 %23°C/50%RH; ISO 62
Water Absorption at Saturation 0.0060 %0.0060 %ISO 62
Linear Mold Shrinkage, Flow 0.00 cm/cm0.00 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 200 MPa29000 psi5mm/min; ISO 527-2/1A
Elongation at Break 3.1 %3.1 %5mm/min; ISO 527-2/1A
Tensile Modulus 11.66 GPa1691 ksi50mm/min; ISO 527-2/1A
Flexural Strength 158 MPa22900 psiISO 178
Flexural Modulus 9.10 GPa1320 ksiISO 178
Izod Impact, Notched (ISO) 95.0 kJ/m²45.2 ft-lb/in²ISO 180/1A
 252 kJ/m²
@Temperature 23.0 °C
120 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched 26.7 J/cm²127 ft-lb/in²ISO 179/1eU
 5.30 J/cm²
@Temperature -30.0 °C
25.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 9.50 J/cm²45.2 ft-lb/in²ISO 179/1eA
Tensile Creep Modulus, 1 hour 9000 MPa1.31e+6 psiISO 899-1
Tensile Creep Modulus, 1000 hours 6600 MPa957000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
IEC 60250
 3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 47.0 kV/mm1190 kV/inIEC 60243-1
Dissipation Factor  0.0159
@Frequency 100 Hz
0.0159
@Frequency 100 Hz
IEC 60250
 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 V150 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 4.00 µm/m-°C2.22 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 38.0 µm/m-°C21.1 µin/in-°FISO 11359-2
Melting Point 280 °C536 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 193 °C379 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 94.0 °C201 °FISO 75-1, -2
Vicat Softening Point 145 °C293 °FISO 306
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 285 - 295 °C545 - 563 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 270 - 280 °C518 - 536 °F
Zone 2 275 - 285 °C527 - 545 °F
Zone 3 280 - 290 °C536 - 554 °F
Zone 4 285 - 295 °C545 - 563 °F
Die Temperature 290 - 300 °C554 - 572 °F
Melt Temperature 285 - 295 °C545 - 563 °F
 293 °C559 °FISO 294
Mold Temperature 60.0 - 120 °C140 - 248 °FISO 294
Injection Velocity 150 mm/sec5.91 in/secISO 294
Drying Temperature >= 150 °C>= 302 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Moisture Content <= 0.010 %<= 0.010 %
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Hold Pressure 48.0 MPa6960 psiISO 294
 50.0 - 150 MPa7250 - 21800 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  80 rpm
@Diameter 40.0 mm
80 rpm
@Diameter 1.57 in
 140 rpm
@Diameter 25.0 mm
140 rpm
@Diameter 0.984 in
 200 rpm
@Diameter 16.0 mm
200 rpm
@Diameter 0.630 in
 
Descriptive Properties
Injection moldingYes
Injection speedvery fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Torlon® 4203 Polyamide-imide (PAI)
Syensqo (Solvay Specialty Polymers) PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP)
RTP Company RTP 3400-3 Liquid Crystal Polymer (LCP), Unfilled
Celanese VECTRA MLX4243 LCP
Celanese VECTRA E130i LCP, 30% Glass Reinforced

PHCQ494 / 178949

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.