MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Visit Zeus Inc. for PTFE Tubing

(Viewing data as-entered. Click here to return)
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Extruded

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.00 - 2.30 g/ccAverage value: 2.17 g/cc Grade Count:61
Water Absorption 0.000 - 0.0100 %Average value: 0.00967 % Grade Count:30
Particle Size 400 - 700 µmAverage value: 504 µm Grade Count:41
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 58.0Average value: 58.0 Grade Count:14
Hardness, Shore A 98.0Average value: 98.0 Grade Count:14
Hardness, Shore D 50.0 - 67.0Average value: 58.2 Grade Count:35
Tensile Strength, Ultimate 13.0 - 55.0 MPaAverage value: 25.6 MPa Grade Count:58
Tensile Strength, Yield 20.0 - 196 MPaAverage value: 131 MPa Grade Count:3
Elongation at Break 70.0 - 600 %Average value: 336 % Grade Count:61
Modulus of Elasticity 0.390 - 0.750 GPaAverage value: 0.599 GPa Grade Count:3
Flexural Modulus 0.275 - 0.700 GPaAverage value: 0.500 GPa Grade Count:30
Compressive Yield Strength 2.00 - 24.1 MPaAverage value: 7.31 MPa Grade Count:10
Flex Crack Resistance 1.00e+6Average value: 1.00e+6 Grade Count:15
Poissons Ratio 0.460Average value: 0.460 Grade Count:14
Izod Impact, Notched 1.87 - 1.89 J/cmAverage value: 1.88 J/cm Grade Count:29
Coefficient of Friction 0.0200 - 0.200Average value: 0.0929 Grade Count:39
Coefficient of Friction, Static 0.0500 - 0.0800Average value: 0.0650 Grade Count:14
K (wear) Factor 10.0 - 5040 x 10-8 mm³/N-MAverage value: 4080 x 10-8 mm³/N-M Grade Count:18
Limiting Pressure Velocity 0.0420 - 0.0876 MPa-m/secAverage value: 0.0642 MPa-m/sec Grade Count:14
Taber Abrasion, mg/1000 Cycles 8.90Average value: 8.90 Grade Count:14
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 - 1.00e+19 ohm-cmAverage value: 9.00e+17 ohm-cm Grade Count:37
Surface Resistance 1.00e+15 - 1.00e+18 ohmAverage value: 8.17e+17 ohm Grade Count:35
Dielectric Constant 2.00 - 2.10Average value: 2.09 Grade Count:31
Dielectric Strength 7.44 - 60.0 kV/mmAverage value: 22.1 kV/mm Grade Count:36
Dissipation Factor 0.000100 - 0.000200Average value: 0.000107 Grade Count:29
Arc Resistance 300 secAverage value: 300 sec Grade Count:28
 
Thermal PropertiesOriginal ValueComments
CTE, linear 75.0 - 790 µm/m-°CAverage value: 294 µm/m-°C Grade Count:20
Specific Heat Capacity 1.50 J/g-°CAverage value: 1.50 J/g-°C Grade Count:14
 1.20 - 1.40 J/g-°C
@Temperature 40.0 - 260 °C
Average value: 1.30 J/g-°C Grade Count:14
Thermal Conductivity 0.167 - 0.300 W/m-KAverage value: 0.292 W/m-K Grade Count:16
Melting Point 321 - 344 °CAverage value: 331 °C Grade Count:32
Maximum Service Temperature, Air 260 - 300 °CAverage value: 261 °C Grade Count:27
Minimum Service Temperature, Air -270 - -79.0 °CAverage value: -183 °C Grade Count:26
Flammability, UL94 V-0Grade Count:31
Oxygen Index 95.0 %Average value: 95.0 % Grade Count:30
 
Processing PropertiesOriginal ValueComments
Processing Temperature 379 - 429 °CAverage value: 404 °C Grade Count:13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded

O1902 / 77907

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.