MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Superior Flux Superior No. 1265 Aluminum Paste Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • A high activity flux designed for low temperature soldering of Aluminum and Aluminum alloys.
  • Paste form ideal for precision dispensing.
  • Effective on joining Aluminum to most ferrous and non-ferrous alloys.
  • Organic-based, chloride-free.
Description: Superior 1265 is a high activity, organic-based, chloride-free, paste Aluminum soldering flux. Applications in which this flux should be used include: Aluminum-to-Aluminum, Aluminum-to-Copper, Aluminum-to-Brass, and Aluminum-to-plated terminals. Its unique paste form makes this flux ideal for applications requiring dispensing or firm adherence of flux to a particular locale. Superior 1265 can also be utilized in joining Aluminum to difficult-to-solder metals like stainless steel, kovar, or nickel. Works effectively with 91Sn/9Zn (Eutectic 199°C/390°F) and other tin/zinc plastic phase alloys; also proven to work effectively with other tin-based solder alloys, such as SN100C and 99.3Sn/0.7Cu.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 9.0 - 109.0 - 1010.6% Solution
Viscosity 300000 - 500000 cP300000 - 500000 cP
 
Thermal PropertiesMetricEnglishComments
Flash Point 180 °C356 °FTCC Method
 
Processing PropertiesMetricEnglishComments
Processing Temperature 177 - 288 °C351 - 550 °FSoldering Range
Shelf Life 2.00 Month2.00 Month
 
Descriptive Properties
FormAmber Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® MH 1657 Polyether Block Amide (PEBA)
Sanyo J-STAT 3180 Antistatic Additive
MetalTek MTEK HC-250 Cast UNS F45009 Abrasion Resistant Cast Iron
Lubrizol Stat-Rite® X-5065 Static Control IDP-TPU Elastomeric Polymer Alloy

NSFLUX092 / 185776

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.