MetalTek MTEK HC-250 Cast UNS F45009 Abrasion Resistant Cast Iron
Categories:
Metal
;
Ferrous Metal
;
Cast Iron
;
Superalloy
;
Iron Base
Material Notes:
Restrict to low stress applications. Resists oxidation and high sulfur flue gas.
Applications: Tuyeres, gas dampers, salt pots, support skids.
Information provided by MetalTek
Key Words:
Cast UNS F45009; Cast Grade CL III TYP A; Cast ASTM A532
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Component Elements Properties
Metric
English
Comments
Carbon, C
2.3 - 3.0 %
2.3 - 3.0 %
Chromium, Cr
23 - 30 %
23 - 30 %
Iron, Fe
58 - 74.7 %
58 - 74.7 %
As Balance
Manganese, Mn
<= 2.0 %
<= 2.0 %
Molybdenum, Mo
<= 3.0 %
<= 3.0 %
Nickel, Ni
<= 2.5 %
<= 2.5 %
Silicon, Si
<= 1.5 %
<= 1.5 %
Descriptive Properties
Heat Treatment
Anneal & Harden
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Class III Type E 25% Cr Martensitic White Cast Iron
UNS F47006 Cast Iron
MetalTek MTEK HC-225 UNS F45005 Abrasion Resistant Cast Iron
MetalTek MTEK 80 Cast UNS F45000 Abrasion Resistant Cast Iron
SAE J431 heavy duty automotive gray cast iron, SAE grade G3500c
NMETEK121 / 18371
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.