MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Master Bond UV15-7DC One Component UV Curable Polymer  (discontinued **)
Categories: Polymer; Thermoset

Material Notes: Replaced by UV15-7DCNV

Key Features:

  • Dual cure: heat & UV light
  • Allows curing in “shadowed out” areas
  • Can be used for potting up to 1/8 inch thick
  • Low shrinkage
Product Description Master: Bond UV15-7DC is a one component, dual cure UV system for high performance bonding, sealing, coating and encapsulation applications. This system features a primary cure utilizing UV light and a secondary cure that requires heating for curing “shadowed out” sections that are not exposed to UV light. The heat required for polymerization is 250-300°F for 15-30 minutes. The UV part of the curing system is most often used for fixturing with the heat curing cycle being added to complete the cure. UV15-7DC has superior physical strength properties, low shrinkage upon cure and good non-yellowing stability. It bonds well to a wide variety of substrates, including glass, metals and many high temperature plastics. This system has very good resistance to chemicals such as water, acids, bases and fuels. UV15-7DC offers excellent dimensional stability, superb electrical insulation properties and a very good capacity to withstand thermal cycling. It has a service temperature range of -80°F to +300°F. UV15-7DC is 100% reactive and does not contain any solvents or other volatiles. The UV part of the cure is not oxygen inhibited and cures readily in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and, of course, the intensity of the light source. As far as the heat curing mechanism, the elevated temperature must reach a minimum of 250°F, as mentioned above. Also, UV15-7DC can even be used for encapsulations up to 1/8 inch thick. However, when used in this manner, the heating should be ramped up slowly (over the course of 30-40 minutes). This system is widely used in optical, fiberoptic, electronic, laser, microelectronic and semiconductor applications.

Product Advantages:

  • One component system; no mixing required
  • Possesses a dual curing mechanism of UV light and heat
  • System capable of rapid fixturing with UV light and curing in “shadowed out” areas by heat
  • Bonds well to a wide variety of substrates
  • Excellent physical strength and electrical insulation properties
  • Can be used for potting up to 1/8 inch thick

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 2000 - 4000 cP
Linear Mold Shrinkage 0.0010 - 0.0020 in/in
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 70
Tensile Strength >= 5000 psi
Tensile Modulus >= 250000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 3.5
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 70.0 µm/m-°C
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -80.0 °F
Glass Transition Temp, Tg 65.0 - 70.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.55
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature <=23.9 °C
in original, unopened containers
 
Descriptive Properties
ColorTransparent

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond UV15 One Component UV Curable Epoxy
Master Bond UV15FL One Component, High Strength, Flexible UV Curable Epoxy
Master Bond UV15-7LRI One Component UV Curable Polymer

PMASTM970 / 185563

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.