MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Master Bond UV15-7LRI One Component UV Curable Polymer
Categories: Polymer; Thermoset

Material Notes: Key Features:
  • One component, fast curing
  • Optically clear
  • Low refractive index
  • Superior dimensional stability
  • Low viscosity
  • Rigid curing
Product Description: Master Bond UV15-7LRI is a one component, low viscosity, UV curable polymer system for bonding, sealing, coating and encapsulating. The system has good physical strength properties; rigid but not brittle. UV15-7LRI cures quickly in 10-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2. The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and of course, the intensity of the light source. UV15-7LRI can cure in sections from 0.080-0.0120 inches deep. However, when bonding, a section of a few thousandths of an inch is more than adequate. UV15-7LRI also possesses excellent electrical insulation properties. It is not oxygen inhibited and therefore does not require any special treatment in that regard. UV15-7LRI is optically clear with excellent light transmission properties. It bonds well to glass, surface treated metals and plastics such as polycarbonates and acrylics, among others. It is especially useful to note that the refractive index is an exceptionally low 1.481. As mentioned above, UV15-7LRI can be cured in sections with thicknesses up to 0.125 inch deep making it well suited for various electronic and opto-electronic potting and encapsulation applications. The system does not contain any solvents or volatiles and none are released during cure. UV15-7LRI offers excellent chemical resistance to water, fuels, acids and bases. Its service temperature range is -60°F to +250°F . Ideal for high production applications where fast fixture times and rapid curing are critical, UV15-7LRI is widely used in fiber-optic, optical, electronic and related industries.

Product Advantages:

  • One component system; no mixing needed; ready to use as supplied
  • Exceptionally fast cure upon exposure to a UV light source at ambient temperatures
  • No air inhibition while curing; no special inert atmosphere required
  • Good electrical insulator
  • Excellent dimensional stability
  • Outstanding optical clarity; excellent light transmission
  • Low refractive index

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 2000 - 4000 cP2000 - 4000 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 55 - 6555 - 65
Tensile Strength 27.6 - 34.5 MPa4000 - 5000 psi
Elongation at Break >= 10 %>= 10 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.8
@Frequency 60 Hz
3.8
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
Glass Transition Temp, Tg 50.0 - 55.0 °C122 - 131 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4811.481
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature <=23.9 °C
6.00 Month
@Temperature <=75.0 °F
in original, unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond UV15 One Component UV Curable Epoxy
Master Bond UV15FL One Component, High Strength, Flexible UV Curable Epoxy
Master Bond UV15-7DC One Component UV Curable Polymer
Esstech X-731-7046 Trifluoroethyl Methacrylate, C6H7O2F3
CHT Group QGel 920 High Refractive Index Silicone Gel

PMASTM971 / 185564

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.