MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay MTM® 58B/58FRB Epoxy Prepreg
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: MTM58FRB is a black pigmented, flame-retarded, 120°C (248°F) curing epoxy prepreg. After an optional post cure, this material can generate a glass transition temperature of 140°C (284°F). MTM58FRB has been developed for component manufacture, particularly automotive structural applications. MTM58FRB is a suitable for autoclave and press molding processes.

Features & Benefits:

  • 60 days out life at 21°C (70°F)
  • 12 months storage at -18°C(0°F)
  • Good hot and wet performance
  • Good impact resistance
  • Excellent tack and drape
  • Recommended cure at 120°C (248°F)
  • MTM58B is flame-retarded and self-extinguishing when tested to FMVS302/ISO3795 and FAR25.857
  • MTM58B is non flame-retarded that meets the self-extinguishing when tested to FMVS302/ISO3795

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.22 g/cc0.0441 lb/in³Cured resin, MTM58B
 1.25 g/cc0.0452 lb/in³Cured resin, MTM58FRB
Storage Temperature -18.0 °C-0.400 °F
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 95.0 °C203 °FDMA E' onset Tg, 1 hr at 120°C, wet
 125 °C257 °FDMA E' onset Tg, 1 hr at 120°C, dry
 140 °C284 °FDMA E' onset Tg, 1 hr at 120°C+2 hrs at 150°C, dry
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay MTM® 57 series Epoxy Matrices
Solvay CYCOM® 381 Epoxy Prepreg with CYCOM 7781 OST E-glass Fabric and 300FAW Epoxy
Solvay CYCOM® 381 Epoxy Prepreg with AS4 Graphite Fabric and 195FAW Epoxy
Solvay CYCOM® 919 Epoxy Prepreg System with Woven E Glass Fiber 7781
Solvay CYCOM® 5216 Epoxy - Unidirectional E-Glass Prepreg

PCYTED151 / 180453

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.