MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay MTM® 57 series Epoxy Matrices
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: MTM57 series resins are toughened, 80 to 120°C (176 to 248°F) curing, epoxy matrices offering flexible processing and a range of handling characteristics. MTM57 series exhibits excellent toughness and, after a suitable cure, can be used at temperatures up to 90°C (1940°F). Qualified to the Federal Motor Vehicle Safety standard no. 302 (flammability of motor vehicle interior materials), and to ISO 3795:1989 (determination of burning behaviors of interior materials for motor vehicles) – when reinforced with 3k carbon fabrics.

Features & Benefits:

  • Versatile processing: autoclave, oven vacuum bag and press molding
  • 30 days out life at 21°C (70°F)
  • 12 months storage at -18°C(0°F)
  • Service temperature up to 90°C (194°F)
  • Flexible curing capability: 80 to 120° (176 to 248°F)
  • MTM57FR & MTM57FRB: self-extinguishing to FAR 25.853(a) flammability specification
  • Cures clear- recommended for cosmetic applications
Product variants:
MTM57S: A MTM57 with equal tack on both sides due to solvent impregnation manufacturing process
MTM57B: Black pigmented variant of MTM57
MTM57OR: Orange pigmented variant of MTM57
MTM57GY: Golden yellow pigmented variant of MTM57
MTM57FR: Flame-retarded variant of MTM57
MTM57FRB: Black pigmented variant of MTM57FR
MTM57-2: Modified tack and improved handling
MTM57-3: Reduced tack for sided impregnation
MTM57-3B: Black pigmented variant of MTM57-3

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³Cured resin, 1 hr at 120°C
 1.38 g/cc0.0499 lb/in³Cured resin, 1 hr at 120°C, FR products
Storage Temperature -18.0 °C-0.400 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °F
Glass Transition Temp, Tg 100 °C212 °FDMA E' onset Tg, 12 hrs at 80°C, dry
 120 °C248 °FDMA E' onset Tg, 3 hrs at 100°C, dry
 125 °C257 °FDMA E' onset Tg, 1 hr at 120°C, dry
 
Processing PropertiesMetricEnglishComments
Cure Time  180 min
@Temperature 100 °C
3.00 hour
@Temperature 212 °F
 720 min
@Temperature 80.0 °C
12.0 hour
@Temperature 176 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay MTM® 58B/58FRB Epoxy Prepreg
Solvay CYCOM® 381 Epoxy Prepreg with CYCOM 7781 OST E-glass Fabric and 300FAW Epoxy
Solvay CYCOM® 919 Epoxy Prepreg System with Woven E Glass Fiber 7781
Solvay Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay CYCOM® 5216 Epoxy - Unidirectional E-Glass Prepreg

PCYTED150 / 180452

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.