MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
IBC Advanced Alloys 21CT C82510 High Strength Beryllium Copper Casting Alloy
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy; Copper Casting Alloy

Material Notes: 21CT has a small titanium addition to produce a finer grained product than 21C.

Information provided by IBC Advanced Alloys.

Key Words: UNS C82510
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.30 g/ccBased on UNS number
 
Thermal PropertiesOriginal ValueComments
Melting Point 1575 - 1800 °F
Solidus 1575 °F
Liquidus 1800 °F
 
Processing PropertiesOriginal ValueComments
Casting Temperature 1800 - 1950 °FPouring Range
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 1.9 - 2.15 %
Cobalt, Co 1.0 - 1.2 %
Copper, Cu 96.2 - 96.88 %As Balance
Silicon, Si 0.20 - 0.35 %
Titanium, Ti 0.02 - 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Materion BrushCAST® 165CT Fine Grain Casting Alloy (As Cast & Aged)
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Brush Wellman Beryllium Copper Alloy 10 Strip; HTC Temper (UNS C17500)
Brush Wellman Beryllium Copper Alloy 165 Strip; 1/2H (TD02) Temper (UNS C17000)
Cadi MOLD-MOR™ 3

NIBCA8251T / 177693

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.