MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik P84®NT Polyimide  (discontinued **)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: Polyimide P84®NT is available in powder or granulate form, which is processable by employing common sinter technologies such as hot compression molding or direct forming. The high mechanical stability and the impact resistance of P84®NT parts ensure good machinability with standard tools. Parts made of Polyimide P84®NT are excellent performers in thermally and mechanically stressed applications.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 140 MPaISO 527
Elongation at Break 10 %ISO 527
Tensile Modulus 3581 MPaISO 527
Compressive Strength 470 MPaISO 604
Compressive Modulus 1960 MPaISO 604
Charpy Impact Unnotched 40.0 kJ/m²ISO 179-1/1eU
Charpy Impact, Notched 6.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 22.0 kV/mmISO 60243-1
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 343 °C
Deflection Temperature at 1.8 MPa (264 psi) 319 °C
Glass Transition Temp, Tg 337 °CDSC

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik P84®NT 15G® Polyimide
Overview of materials for Polyimide
Overview of materials for Polyimide, Thermoset Film
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
Overview of materials for Thermoplastic Polyimide, Unfilled

PEVONIL153 / 196357

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.