MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials VESPEL TP-8054 Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: DuPont Vespel TP-8054 parts are specified for high-temperature applications requiring a balance of mechanical and thermal properties. TP-8054 parts are produced from unreinforced thermoplastic polyimide (TPI).

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc
@Temperature 23.0 °C
1.33 g/cc
@Temperature 73.4 °F
ASTM D792
Moisture Absorption  0.24 %
@Temperature 23.0 °C
0.24 %
@Temperature 73.4 °F
60%RH,23°C,24h; ASTM D570
 0.34 %
@Temperature 23.0 °C
0.34 %
@Temperature 73.4 °F
50%RH,23°C,24h; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 47
@Temperature 23.0 °C
47
@Temperature 73.4 °F
ASTM D785
Tensile Strength  58.0 MPa
@Temperature 150 °C
8410 psi
@Temperature 302 °F
ASTM D638
 92.0 MPa
@Temperature 23.0 °C
13300 psi
@Temperature 73.4 °F
ASTM D638
Elongation at Break  90 %
@Temperature 23.0 °C
90 %
@Temperature 73.4 °F
ASTM D638
 90 %
@Temperature 150 °C
90 %
@Temperature 302 °F
ASTM D638
Flexural Strength  88.0 MPa
@Temperature 150 °C
12800 psi
@Temperature 302 °F
ASTM D790
 137 MPa
@Temperature 23.0 °C
19900 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus  2.60 GPa
@Temperature 150 °C
377 ksi
@Temperature 302 °F
ASTM D790
 2.90 GPa
@Temperature 23.0 °C
421 ksi
@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 0.900 J/cm
@Temperature 23.0 °C
1.69 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 - 1.00e+18 ohm-cm
@Temperature 23.0 °C
1.00e+17 - 1.00e+18 ohm-cm
@Temperature 73.4 °F
ASTM D257
Surface Resistance 1.00e+15 - 1.00e+16 ohm
@Temperature 23.0 °C
1.00e+15 - 1.00e+16 ohm
@Temperature 73.4 °F
ASTM D257
Dielectric Constant  3.1
@Frequency 1e+6 Hz,
Temperature 23.0 °C
3.1
@Frequency 1e+6 Hz,
Temperature 73.4 °F
ASTM D150
 3.2
@Frequency 10000 Hz,
Temperature 23.0 °C
3.2
@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D150
Dissipation Factor  0.00090
@Frequency 10000 Hz,
Temperature 23.0 °C
0.00090
@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D150
 0.0034
@Frequency 1e+6 Hz,
Temperature 23.0 °C
0.0034
@Frequency 1e+6 Hz,
Temperature 73.4 °F
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 238 °C460 °FASTM D648
 
Descriptive Properties
AppearanceNatural Color
FormsShapes
Material StatusCurrent
Region Available - GlobalYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials VESPEL TP-8130 Polyimide
Overview of materials for Polyimide
DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
DuPont Mobility and Materials VESPEL TP-8161 Polyimide
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight

PDSZ1269 / 140086

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.