MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

DuPont Mobility and Materials VESPEL TP-8161 Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: DuPont Vespel TP-8161 parts are specified for high-temperature applications. TP-8161 parts offer a unique balance of mechanical and thermal properties for superior performance in aggressive environments. TP-8161 parts are produced from unfilled thermoplas

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc
@Temperature 23.0 °C
1.35 g/cc
@Temperature 73.4 °F
ASTM D792
Moisture Absorption  0.070 %
@Temperature 23.0 °C
0.070 %
@Temperature 73.4 °F
60%RH,23°C,24h; ASTM D570
 0.16 %
@Temperature 23.0 °C
0.16 %
@Temperature 73.4 °F
50%RH,23°C,24h; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 80.0 MPa
@Temperature 23.0 °C
11600 psi
@Temperature 73.4 °F
ASTM D638
Elongation at Break 3.0 %
@Temperature 23.0 °C
3.0 %
@Temperature 73.4 °F
ASTM D638
Flexural Strength 154 MPa
@Temperature 23.0 °C
22300 psi
@Temperature 73.4 °F
ASTM D790
Flexural Modulus 4.20 GPa
@Temperature 23.0 °C
609 ksi
@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 0.370 J/cm
@Temperature 23.0 °C
0.693 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+17 - 1.00e+18 ohm-cm
@Temperature 23.0 °C
1.00e+17 - 1.00e+18 ohm-cm
@Temperature 73.4 °F
ASTM D257
Surface Resistance 1.00e+15 - 1.00e+16 ohm
@Temperature 23.0 °C
1.00e+15 - 1.00e+16 ohm
@Temperature 73.4 °F
ASTM D257
Dielectric Constant  3.1
@Frequency 1e+6 Hz,
Temperature 23.0 °C
3.1
@Frequency 1e+6 Hz,
Temperature 73.4 °F
ASTM D150
 3.2
@Frequency 10000 Hz,
Temperature 23.0 °C
3.2
@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D150
Dissipation Factor  0.00090
@Frequency 10000 Hz,
Temperature 23.0 °C
0.00090
@Frequency 10000 Hz,
Temperature 73.4 °F
ASTM D150
 0.0030
@Frequency 1e+6 Hz,
Temperature 23.0 °C
0.0030
@Frequency 1e+6 Hz,
Temperature 73.4 °F
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 295 °C563 °FASTM D648
Flammability, UL94  V-0
@Thickness 0.400 mm
V-0
@Thickness 0.0157 in
DAM; UL94
 5VA
@Thickness 2.00 mm
5VA
@Thickness 0.0787 in
DAM; UL94
Oxygen Index 47 %47 %ASTM D2863
 
Descriptive Properties
AppearanceNatural Color
FormsShapes
Material StatusCurrent
Region Available - GlobalYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polytetrafluoroethylene (PTFE), Molded
Overview of materials for Nylon 6, Cast
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Direct formed
Overview of materials for Nylon 6, Extruded
DuPont Mobility and Materials VESPEL TP-8130 Polyimide

PDSZ1271 / 140088

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.