MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zotefoams Evazote® EV30 Ethylene Vinyl Acetate Copolymer Foam
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.

Information provided by Zotefoams

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0300 g/cc0.00108 lb/in³Nominal skin/skin; BS ISO 7214 1998
 0.0280 - 0.0380 g/cc0.00101 - 0.00137 lb/in³sheet density
Cell Length 0.450 mm0.0177 inTypical Diameter
 0.300 - 0.700 mm0.0118 - 0.0276 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 383810 mm cell/cell thickness; ISO 868 1985
Tensile Strength 0.615 MPa89.2 psiISO 7214 1998
Elongation at Break 190 %190 %
Compressive Yield Strength  0.0200 MPa
@Strain 10 %
2.90 psi
@Strain 10 %
BS ISO 7214 1998
 0.0370 MPa
@Strain 25 %
5.37 psi
@Strain 25 %
BS ISO 7214 1998
 0.0670 MPa
@Strain 40 %
9.72 psi
@Strain 40 %
BS ISO 7214 1998
 0.0960 MPa
@Strain 50 %
13.9 psi
@Strain 50 %
BS ISO 7214 1998
Tear Strength 0.630 kN/m3.59 pliBS EN ISO 8067 1995
Compression Set  5.0 %
@Time 79200 sec,
Strain 25 %
5.0 %
@Time 22.0 hour,
Strain 25 %
24 hr recovery; BS ISO 7214 1998
 14 %
@Time 79200 sec,
Strain 25 %
14 %
@Time 22.0 hour,
Strain 25 %
0.5 hr recovery; BS ISO 7214 1998
 19 %
@Time 79200 sec,
Strain 50 %
19 %
@Time 22.0 hour,
Strain 50 %
24 hr recovery; BS ISO 7214 1998
 29 %
@Time 79200 sec,
Strain 50 %
29 %
@Time 22.0 hour,
Strain 50 %
0.5 hr recovery; BS ISO 7214 1998
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0402 W/m-K0.279 BTU-in/hr-ft²-°Fmean temp of 10°C; ISO 8302 1991
Maximum Service Temperature, Air 65.0 °C149 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Flammability Test  0.80
@Thickness 13.0 mm
0.80
@Thickness 0.512 in
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 1.3
@Thickness 5.00 mm
1.3
@Thickness 0.197 in
Horizontal Burn Rate, mm/sec; ISO 7214 1998
 
Descriptive Properties
FlammabilityAutomotive: FMVSS.302 burn ratePass: 6mm and thicker

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam
Zotefoams Plastazote® HD30 High Density Polyethylene Foam
Micropol E188 Rotational molding powder based on a random EVA copolymer
LyondellBasell Lupolen V 3520 K Ethylene Vinyl Acetate

PZOTEF943 / 150699

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.