MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Micropol E188 Rotational molding powder based on a random EVA copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Information provided by Micropol Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D1505
Vinyl Acetate Content 18 %18 %by weight
Melt Flow 8.0 g/10 min8.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 3535ASTM S2240
Tensile Strength, Yield 3.50 MPa508 psiASTM D638
Elongation at Break 700 %700 %ASTM D638
Modulus of Elasticity 0.0500 GPa7.25 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 61.0 °C142 °F1kg load; ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Innospec FLEXAREN® 07002 EVA-Copolymer
Innospec FLEXAREN® 07000 EVA-Copolymer
Micropol Microcoat DG/EVA/214A Microground modified EVA copolymer
Westlake EB502 12.5% EVA Copolymer
Westlake Elevate™ EB591 9% EVA Copolymer

PMICRO17 / 53074

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.