MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Tropical American Mahogany Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Diffuse-Porous. Excellent shaping, very good planing, fair steam bending. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Durable (15 to 25 years)
Resistance to penetration by preservatives: Extremely resistant
Common Applications: Furniture, cabinet work, interior and exterior joinery. Boat building

Key Words: Swietenia macrophylla; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.450 g/cc0.450 g/ccGreen
Density 0.600 g/cc0.0217 lb/in³Air Dry (12-15% Moisture Content)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 3300 N742 lb (f)Side Hardness, Green
 3600 N809 lb (f)Side Hardness, 12% Moisture
Tensile Strength, Ultimate 2.40 MPa348 psiPerpendicular to Grain
Modulus of Rupture 0.0621 GPa9.01 ksiStatic Bending, Green
 0.0770 GPa11.2 ksiIn Bending
 0.0793 GPa11.5 ksiStatic Bending, 12% Moisture
Flexural Modulus 8.33 - 9.86 GPa1210 - 1430 ksiIn Bending
 9.20 GPa1330 ksiStatic Bending, Green
 10.3 GPa1490 ksiStatic Bending, 12% Moisture
Compressive Strength 8.30 MPa1200 psiPerpendicular to Grain
 29.9 MPa4340 psiParallel to Grain, Green
 44.1 - 49.0 MPa6400 - 7110 psiParallel to Grain
 46.7 MPa6770 psiParallel to Grain, 12% Moisture
Poissons Ratio 0.0330.033µRL, 12% Moisture Content
 0.0340.034µTL, 12% Moisture Content
 0.3140.314µLR, 12% Moisture Content
 0.3260.326µTR, 12% Moisture Content
 0.5330.533µLT, 12% Moisture Content
 0.600.60µRT, 12% Moisture Content
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 8.50 MPa1230 psiParallel to Grain, Green
 8.50 MPa1230 psiParallel to Grain, 12% Moisture
Impact 5.25.2J/cm² Toughness
Work to Maximum Load 0.0520 J/cm³7.54 in-lb/in³Static Bending, 12% Moisture
 0.0630 J/cm³9.14 in-lb/in³Static Bending, Green
 
Thermal PropertiesMetricEnglishComments
Shrinkage 3.0 %3.0 %Radial Shrinkage Green to Oven Dry
 4.1 %4.1 %Tangential Shrinkage Green to Oven Dry
 7.8 %7.8 %Volumetric Shrinkage Green to Oven Dry
 
Descriptive Properties
ColorReddish-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
African Mahogany Wood
Teak Wood
American Red Oak Wood
American Coast Douglas Fir Wood
American Maple, Rock (Sugar Maple)

PTSID / 71347

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.