MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

American Red Oak Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Ring-Porous Hardwood. Least easy to work with hand tools. Excellent steam bending, excellent planing, fair shaping. Data is based on small, clear, air-dried samples unless specified.

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Quercus rubra; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.560 g/cc0.0202 lb/in³Oven Dry Weight/Unseasoned Volume
 0.610 g/cc0.0220 lb/in³at 12% moisture content
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 4200 N944 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 4500 N1010 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 5.10 MPa740 psiPerpendicular to Grain*
 5.50 MPa798 psiPerpendicular to Grain
Modulus of Rupture 0.0531 GPa7.70 ksiStatic Bending*
 0.0990 GPa14.4 ksiIn Bending
Flexural Yield Strength 25.5 MPa3700 psiFiber Stress at Elastic Limit; Static Bending*
 57.9 MPa8400 psiBending stress at proportional limit
Flexural Modulus 8.89 GPa1290 ksiStatic Bending*
 12.4 - 12.56 GPa1800 - 1822 ksiIn Bending
Compressive Strength 5.03 MPa730 psiPerpendicular to Grain*
 8.60 MPa1250 psiPerpendicular to Grain
 16.1 MPa2330 psiParallel to Grain*
 22.1 MPa3200 psiMax Crushing Strength Parallel to Grain*
 47.0 - 48.9 MPa6820 - 7090 psiParallel to Grain
Poissons Ratio 0.0330.033µTL, 12% Moisture Content
 0.0640.064µRL, 12% Moisture Content
 0.2920.292µTR, 12% Moisture Content
 0.350.35µLR, 12% Moisture Content
 0.4480.448µLT, 12% Moisture Content
 0.560.56µRT, 12% Moisture Content
Shear Strength 7.72 MPa1120 psiParallel to Grain*
Impact 3.93.9in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 1040010400psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00448 J/cm³0.650 in-lb/in³Static Bending*
Work to Maximum Load 0.0793 J/cm³11.5 in-lb/in³Static Bending*
Cleavage 67.0 kN/m382 lb/inRadial surface of failure, Unseasoned*
 82.0 kN/m468 lb/inTangential surface of failure, Unseasoned*
 
Thermal PropertiesMetricEnglishComments
CTE, linear  4.90 µm/m-°C
@Temperature 20.0 °C
2.72 µin/in-°F
@Temperature 68.0 °F
Axial. Typical value for Oak.
 11.1 µm/m-°C
@Temperature 20.0 °C
6.17 µin/in-°F
@Temperature 68.0 °F
Radial; Typical value for Oak.
 54.4 µm/m-°C
@Temperature 20.0 °C
30.2 µin/in-°F
@Temperature 68.0 °F
Tangential. Typical value for Oak.
Shrinkage 2.05 %2.05 %Tangential; Unseasoned to Oven Dry*
 4.0 %4.0 %Volumetric; Unseasoned to Oven Dry*
 8.2 %8.2 %Radial; Unseasoned to Oven Dry*

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American White Oak Wood
European Red Oak Wood
North American Northern Red Oak Wood
Laurel Red Oak Wood
Pin Red Oak Wood

PTSAV / 71305

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.