MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2)
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Speed Star high speed steel in a fine-grained "Moly"-Tungsten high-speed steel manufactured under close control. It has certain advantages over 18-4-1 high speed steels, some of which are lower cost, less weight per cubic inch, lower hardening temperature and somewhat easier machining.

Applications: Lathe tools, Planer tools, Drills, Taps, Reamers, Broaches, Milling cutters, Form cutters, Thread chasers, End mills, Gear cutters, Wood knives

Information provided by Carpenter Technology Corporation.

Speed Star® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS T11302
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 8.15 g/cc8.15 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 6262Tempered at 1150°F, Quenched at 2200°F
 6565As hardened, Quenched at 2200°F
Compressive Yield Strength 3250 MPa471000 psiwhen tempered at 300°F
Izod Impact Unnotched 67.0 J49.4 ft-lbwhen tempered at 300°F
Abrasion 25.825.8loss in mm3, As-Hardened; ASTM G65
 77.777.7loss in mm3, Tempered at 1275°F; ASTM G65
 
Thermal PropertiesMetricEnglishComments
CTE, linear  10.0 µm/m-°C
@Temperature 20.0 - 100 °C
5.56 µin/in-°F
@Temperature 68.0 - 212 °F
 12.2 µm/m-°C
@Temperature 20.0 - 500 °C
6.78 µin/in-°F
@Temperature 68.0 - 932 °F
 12.6 µm/m-°C
@Temperature 20.0 - 850 °C
7.00 µin/in-°F
@Temperature 68.0 - 1560 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.82 %0.82 %
Chromium, Cr 4.25 %4.25 %
Iron, Fe 81.33 %81.33 %As Balance
Manganese, Mn 0.30 %0.30 %
Molybdenum, Mo 5.0 %5.0 %
Silicon, Si 0.25 %0.25 %
Tungsten, W 6.25 %6.25 %
Vanadium, V 1.8 %1.8 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Crucible Steel Rex M2 High Speed Steel
Crucible Steel PM M2 Tool Steel
Crucible Steel REX® M2 S 1.0C High Speed Steel, AISI M2
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel

NCARN21 / 15860

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.