MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel Rex M2 High Speed Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Rex M2 is a tungsten-molybdenum general purpose high speed steel. It is suitable for a wide variety of cutting tools and is often used for metalforming tools such as punches and dies. Rex M2 is a good choice for cutting tools which require moderate feeds and speeds. It provides sufficient red hardness along with outstanding toughness for a high speed steel. For cold work applications, Rex M2 offers higher hardness and wear resistance than D2. Its high attainable hardness provides superior compressive strength for deformation resistance, reducing susceptibility to such problems as peening, denting and edge rollover. Its high tempering temperature and red hardness make it an excellent substrate for most surface treatments.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.14 g/cc0.294 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 217 - 255217 - 255Annealed
Hardness, Rockwell C 6161Austenitizing Temperature- 1150°C; Tempering Temperature- 580°C
 6464Austenitizing Temperature- 1190°C; Tempering Temperature- 550°C
Modulus of Elasticity 207 GPa30000 ksi
Charpy Impact 23.0 J17.0 ft-lbAustenitizing Temperature- 1190°C; Tempering Temperature- 550°C
 28.0 J20.7 ft-lbAustenitizing Temperature- 1150°C; Tempering Temperature- 580°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.3 µm/m-°C
@Temperature 40.0 - 260 °C
6.28 µin/in-°F
@Temperature 104 - 500 °F
 12.5 µm/m-°C
@Temperature 40.0 - 540 °C
6.94 µin/in-°F
@Temperature 104 - 1000 °F
Shrinkage -0.220 - -0.150 %-0.220 - -0.150 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.85 %0.85 %
Chromium, Cr 4.15 %4.15 %
Iron, Fe 81.65 %81.65 %As Remainder
Molybdenum, Mo 5.0 %5.0 %
Tungsten, W 6.4 %6.4 %
Vanadium, V 1.95 %1.95 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Crucible Steel PM M2 Tool Steel
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2)
Latrobe Double Six™ ASTM M2 High Speed Steel
Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications

NCRUC014 / 16007

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.