MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Cold Work Steel

Material Notes: Properties: Tungs ten-molybdenum high speed steel with ex cel lent toughness and cut ting proper ties, for a wide variety of uses.

Applications: Taps, twist drills, reamers, broaching tools, metal saws, milling tools of all types, wood working tools, cold work tools.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.10 g/cc0.293 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 217 GPa31500 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000540 ohm-cm0.0000540 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 - 100 °C
6.39 µin/in-°F
@Temperature 68.0 - 212 °F
 11.7 µm/m-°C
@Temperature 20.0 - 200 °C
6.50 µin/in-°F
@Temperature 68.0 - 392 °F
 12.2 µm/m-°C
@Temperature 20.0 - 300 °C
6.78 µin/in-°F
@Temperature 68.0 - 572 °F
 12.4 µm/m-°C
@Temperature 20.0 - 400 °C
6.89 µin/in-°F
@Temperature 68.0 - 752 °F
 12.7 µm/m-°C
@Temperature 20.0 - 500 °C
7.06 µin/in-°F
@Temperature 68.0 - 932 °F
 12.9 µm/m-°C
@Temperature 20.0 - 700 °C
7.17 µin/in-°F
@Temperature 68.0 - 1290 °F
 13.0 µm/m-°C
@Temperature 20.0 - 600 °C
7.22 µin/in-°F
@Temperature 68.0 - 1110 °F
Specific Heat Capacity 0.460 J/g-°C0.110 BTU/lb-°F
Thermal Conductivity 19.0 W/m-K132 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.85 %0.85 %
Chromium, Cr 4.1 %4.1 %
Iron, Fe 81.15 %81.15 %As Balance
Manganese, Mn 0.25 %0.25 %
Molybdenum, Mo 5.0 %5.0 %
Silicon, Si 0.35 %0.35 %
Tungsten, W 6.4 %6.4 %
Vanadium, V 1.9 %1.9 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2)
Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel
Crucible Steel Rex M2 High Speed Steel
Crucible Steel PM M2 Tool Steel

NBUCOR22 / 15491

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.