MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Bohler-Uddeholm UDDEHOLM VANADIS 30 AISI M2 + Co SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Cold Work Steel

Material Notes: Uddeholm Vanadis 30 is a Co high alloyed powder metallurgy high speed steel corresponding to AISI M3:2 + Co. The high compressive strength, 67 HRC, and good abrasive wear resistance makes Uddeholm Vanadis 30 suitable for demanding cold work applications and for cutting tools as an alternative to AISI M42 or other Co-alloyed HSS. The P/M process gives a good machinability and grindability as well as a good dimension stability during heat treatment.

Vanadis 30 is characterized by:

  • High wear resistance
  • High compressive strength at high hardness
  • Good through hardening properties
  • Good toughness
  • Good dimensional stability on heat treatment
  • Good machinability and grindability
  • Very good temper resistance
Uddeholm Vanadis 30 is a cobalt alloyed high performance PM high speed steel. The cobalt addition of approx. 8,5% has a positive influence on the hot strength/hot hardness, temper resistance and modulus of elasticity. The presence of cobalt has little influence on wear resistance. As cobalt does not form carbides, the wear resistance of Uddeholm Vanadis 30 is more or less the same as for steels with the same base analysis but without cobalt (e.g. Uddeholm Vanadis 23). On the other hand, its presence reduces the toughness and hardenability somewhat but increases compressive strength and high temperature properties.
    For cold work:
  • The combination of high wear resistance and unusually good compressive strength can be put to use in tooling for heavy forming operations.
  • In some cold work operations, the active surface (e.g. cutting edge or forming surface) of a tool can reach temperatures in excess of 200°C (390°F). Such conditions can be found in tooling running on high speed presses. Also, development of high temperatures in the tooling can be expected in heavy forming operations.

Key Words: W.-Nr. 1.3207
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.94 g/cc0.287 lb/in³soft annealed
 7.86 g/cc
@Temperature 600.0 °C
0.284 lb/in³
@Temperature 1112 °F
soft annealed
 7.89 g/cc
@Temperature 399 °C
0.285 lb/in³
@Temperature 750 °F
soft annealed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 300<= 300Soft annealed
 <= 320<= 320Drawn
Hardness, Rockwell C 60 - 6760 - 67austenitizing 1832-2156°F, temper 3 x 1hr at 1040°F
Modulus of Elasticity 234 GPa34000 ksi(hardened and tempered)
 193 GPa
@Temperature 600.0 °C
28000 ksi
@Temperature 1112 °F
hardened and tempered
 214 GPa
@Temperature 399 °C
31000 ksi
@Temperature 750 °F
hardened and tempered
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.7 µm/m-°C
@Temperature 399 °C
6.50 µin/in-°F
@Temperature 750 °F
hardened and tempered
 12.2 µm/m-°C
@Temperature 600.0 °C
6.80 µin/in-°F
@Temperature 1112 °F
hardened and tempered
Specific Heat Capacity  0.418 J/g-°C
@Temperature 20.0 °C
0.100 BTU/lb-°F
@Temperature 68.0 °F
hardened and tempered
 0.502 J/g-°C
@Temperature 399 °C
0.120 BTU/lb-°F
@Temperature 750 °F
hardened and tempered
 0.586 J/g-°C
@Temperature 600.0 °C
0.140 BTU/lb-°F
@Temperature 1112 °F
hardened and tempered
Thermal Conductivity  22.0 W/m-K
@Temperature 20.0 °C
153 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
hardened and tempered
 25.0 W/m-K
@Temperature 600.0 °C
174 BTU-in/hr-ft²-°F
@Temperature 1112 °F
hardened and tempered
 26.0 W/m-K
@Temperature 399 °C
180 BTU-in/hr-ft²-°F
@Temperature 750 °F
hardened and tempered
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.28 %1.28 %
Chromium, Cr 4.2 %4.2 %
Cobalt, Co 8.5 %8.5 %
Iron, Fe 71.5 %71.5 %As Balance
Molybdenum, Mo 5.0 %5.0 %
Tungsten, W 6.4 %6.4 %
Vanadium, V 3.1 %3.1 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type M2 Molybdenum High Speed Tool Steel (UNS T11302)
ATI Allegheny Ludlum M2 Tool Steel, UNS T11302
Carpenter Speed Star® High Speed Steel (Red-Hard) (AISI M2)
Bohler-Uddeholm BÖHLER S601 (M2 Modified) High Speed Steel For Cold Work Applications
Crucible Steel REX® M2 S 1.0C High Speed Steel, AISI M2

NBUCOR16 / 15485

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.