MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Essentium TPU 90A Additive Manufacturing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Essentium TPU 90A filament exhibits excellent interlayer adhesion and high stain at break. Provides flexibility, grip, and abrasion resistance. Applications: flexible hinges, belts, plugs, gaskets, protective cases, overgrips, wheels, shoe soles, vibration dampeners, energy absorbing lattices, etc.

Definitions of axes used in property data table: XY is the print direction. ZX is the build direction. YX is the third orthogonal axis.

Information provided by Essentium Materials, LLC.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccMolded; ISO 1183
Melt Flow 30 - 50 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D 2240
Tensile Strength 17.0 MPaZX; ASTM D 412
 25.0 MPaYX; ASTM D 412
 32.0 MPaXY; ASTM D 412
 37.0 MPa45°-45°; ASTM D 412
 44.0 MPaMolded; ASTM D 412
Tensile Modulus 416 MPaZX; ASTM D 412
 520 MPaMolded; ASTM D 412
 630 MPaYX; ASTM D 412
 710 MPaXY; ASTM D 412
 844 MPa45°-45°; ASTM D 412
100% Modulus 0.00700 GPa
@Strain 100 %
45°-45°; ASTM D 412
 0.00700 GPa
@Strain 100 %
YX; ASTM D 412
 0.00700 GPa
@Strain 100 %
ZX; ASTM D 412
 0.00800 GPa
@Strain 100 %
XY; ASTM D 412
 0.0100 GPa
@Strain 100 %
Molded; ASTM D 412
300% Modulus 0.0130 GPa
@Strain 300 %
YX; ASTM D 412
 0.0130 GPa
@Strain 300 %
ZX; ASTM D 412
 0.0140 GPa
@Strain 300 %
45°-45°; ASTM D 412
 0.0140 GPa
@Strain 300 %
XY; ASTM D 412
 0.0230 GPa
@Strain 300 %
Molded; ASTM D 412
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 128 °CASTM D 1525
Glass Transition Temp, Tg -30.0 °CInternal
 
Processing PropertiesOriginal ValueComments
Processing Temperature 205 - 250 °CExtrusion Temperature
Nozzle Temperature 240 °C
 
Descriptive Properties
Bed Temperature, °C23-60
Enclosure Temperature, °CRoom Temperature
Print SettingsInfill.: 100%; 20 mm/s, layer height: 0.3mm, extrusion multiplier: 1.05, nozzle diameter: 1.0 mm
Print Speed, mm/s15-30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Essentium High Performance PLA Additive Manufacturing Filament
Clariant Polylactic Acid Black 3D Printer Filament
Clariant Acrylonitrile Butadiene Styrene Black 3D Printer Filament
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Eastman Eastar GN007 PETG Copolyester

PESSEN907 / 220995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.