MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Essentium TPU 90A Additive Manufacturing Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Essentium TPU 90A filament exhibits excellent interlayer adhesion and high stain at break. Provides flexibility, grip, and abrasion resistance. Applications: flexible hinges, belts, plugs, gaskets, protective cases, overgrips, wheels, shoe soles, vibration dampeners, energy absorbing lattices, etc.

Definitions of axes used in property data table: XY is the print direction. ZX is the build direction. YX is the third orthogonal axis.

Information provided by Essentium Materials, LLC.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.21 g/cc0.0437 lb/in³Molded; ISO 1183
Melt Flow 30 - 50 g/10 min
@Load 2.16 kg,
Temperature 210 °C
30 - 50 g/10 min
@Load 4.76 lb,
Temperature 410 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D 2240
Tensile Strength 17.0 MPa2470 psiZX; ASTM D 412
 25.0 MPa3630 psiYX; ASTM D 412
 32.0 MPa4640 psiXY; ASTM D 412
 37.0 MPa5370 psi45°-45°; ASTM D 412
 44.0 MPa6380 psiMolded; ASTM D 412
Tensile Modulus 0.416 GPa60.3 ksiZX; ASTM D 412
 0.520 GPa75.4 ksiMolded; ASTM D 412
 0.630 GPa91.4 ksiYX; ASTM D 412
 0.710 GPa103 ksiXY; ASTM D 412
 0.844 GPa122 ksi45°-45°; ASTM D 412
100% Modulus  7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
45°-45°; ASTM D 412
 7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
YX; ASTM D 412
 7.00 MPa
@Strain 100 %
1020 psi
@Strain 100 %
ZX; ASTM D 412
 8.00 MPa
@Strain 100 %
1160 psi
@Strain 100 %
XY; ASTM D 412
 10.0 MPa
@Strain 100 %
1450 psi
@Strain 100 %
Molded; ASTM D 412
300% Modulus  13.0 MPa
@Strain 300 %
1890 psi
@Strain 300 %
YX; ASTM D 412
 13.0 MPa
@Strain 300 %
1890 psi
@Strain 300 %
ZX; ASTM D 412
 14.0 MPa
@Strain 300 %
2030 psi
@Strain 300 %
45°-45°; ASTM D 412
 14.0 MPa
@Strain 300 %
2030 psi
@Strain 300 %
XY; ASTM D 412
 23.0 MPa
@Strain 300 %
3340 psi
@Strain 300 %
Molded; ASTM D 412
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 128 °C262 °FASTM D 1525
Glass Transition Temp, Tg -30.0 °C-22.0 °FInternal
 
Processing PropertiesMetricEnglishComments
Processing Temperature 205 - 250 °C401 - 482 °FExtrusion Temperature
Nozzle Temperature 240 °C464 °F
 
Descriptive Properties
Bed Temperature, °C23-60
Enclosure Temperature, °CRoom Temperature
Print SettingsInfill.: 100%; 20 mm/s, layer height: 0.3mm, extrusion multiplier: 1.05, nozzle diameter: 1.0 mm
Print Speed, mm/s15-30

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Essentium High Performance PLA Additive Manufacturing Filament
Clariant Polylactic Acid Black 3D Printer Filament
Clariant Acrylonitrile Butadiene Styrene Black 3D Printer Filament
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Eastman Eastar GN007 PETG Copolyester

PESSEN907 / 220995

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.